Material Notes:
Information provided by American Precision Prototyping, LLC
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength, Ultimate 4.36 MPa
632 psi
ASTM D412
Elongation at Break 47 %
47 %
ASTM D412
Tear Strength 9.31 kN/m
53.1 pli
ASTM D624
Compression Set 1.0 %
1.0 %
ASTM D395
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 2.60 °C
36.7 °F
DSC (-80°C+100°C)