Material Notes:
Molecular Formula: C40H64O4N4Cas No.: 23128-74-7Use: This product is a non-color-degrading, nonpolluting, heat-resisting, extraction-resisting, high-performance all-purpose antioxidant, mainly applied to polyamnamee, polyolefin, polystyrene, ABS resin, polyacetal resin, acetal resin, polyurethane, as well as rubber etc., it can also be used with auxiliary antioxidant with the general dosage of 0.3-1.0%Package, Storage and Transportation: Stable performance; keep away from high temperature and moisture during storage; packed in paperboard barrel lined with plastic bag.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 155 - 161 °C
311 - 322 °F
Optical Properties Metric English Comments
Transmission, Visible 97 %

@Wavelength 425 nm
97 %

@Wavelength 425 nm
98 %

@Wavelength 500 nm
98 %

@Wavelength 500 nm
Descriptive Properties Value Comments
Appearance White Powder
CAS Number 23128-74-7
Chemical Name N,N'-bis(3-(3,5-diterbutyl-4-hydroxphenyl) propionyl) hexanediamine
Content (%) >98
Molecular Formula C40H64O4N4