Oceanchem Group Antioxidant 168

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Antioxidant 168.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: C42H63O3PCas No.: 31570-04-4Characteristics and Uses: This product is an excellent antioxidant namely applied to polyethylene, polypropylene, polyoxymethylene, ABS resin, PS resin, PVC, engineering plastics, binding agent, rubber, petroleum etc. for product polymerization.Storing and Packing: This product is nontoxic, inflammable, noncorrodible and stable in storing, packed in cardboard pail lined with plastic bags with the net capacity of 25 kg per pail.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Volatiles <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 182 - 185 °C
360 - 365 °F
Optical Properties Metric English Comments
Transmission, Visible >= 97 %

@Wavelength 425 nm
>= 97 %

@Wavelength 425 nm
10g/100ml Toluene; clarified at room temperature
>= 97 %

@Wavelength 500 nm
>= 97 %

@Wavelength 500 nm
10g/100ml Toluene; clarified at room temperature
Descriptive Properties Value Comments
Appearance White crystalline powder
CAS Number 31570-04-4
Chemical Name Tri(2,4-Tertbutylphenyl)Phosphorite
Content (%) >99.0
Ethyl Acetate (%) 11
4% Ethane (20°C, W/W)
36
Cycloehane
Methanol (%) <0.01
Water
36
Dichloromethane
Molecular Formula C42H63O3P
Solubility 0.01
Acetone
0.34
Benzene
0.36
Chloroform