Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oceanchem Group Brominated Polystyrene (BPS)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Brominated Polystyrene (BPS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: (C8H5Br3)nCas No.: 88497-56-7Application: Mainly used for PBT, PET and PA as flame-retardant.Information Provided by Oceanchem Group
Thermal Properties Metric English Comments
Melting Point 260 - 320 °C
500 - 608 °F
Descriptive Properties Value Comments
Appearance Gray powder
Bromine, Br (%) 66-68
CAS Number 88497-56-7
Intenerating Point (°C) 210-250
Molecular Formula (C8H5Br3)n
Users viewing this material also viewed the following: