Oceanchem Group Decabromodiphenyl Ethane (DBDPE/8010)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Decabromodiphenyl Ethane (DBDPE/8010).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: C14Br10H4Cas No.: 84852-53-9Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: This product is a new high efficiency, environmentally friendly flame retardant developed by our company and Beijing Institute of Technology. The product has properties of high bromine content, excellent thermal stability, low toxicity and UV-resistance. It is used in high-impact polystyrene, engineering plastics, wires and cables, insulator, elastomer and thermoset plastics etc.Storage and Transportation: Handle with care, keep air-tight and dry.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Volatiles <= 0.10 %
<= 0.10 %
Particle Size <= 3.0 µm
<= 3.0 µm
Best Grade
<= 5.0 µm
<= 5.0 µm
Grade I
Molecular Weight 971.22 g/mol
971.22 g/mol
Thermal Properties Metric English Comments
Melting Point 340 °C
644 °F
Descriptive Properties Value Comments
Bromine, Br (%) 81-82
CAS Number 84852-53-9
Free Br (ppm) <10
Molecular Formula C14Br10H4
Whiteness >85
Grade I
>87
Best Grade