Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oceanchem Group Resorcinol bis (Diphenyl Phosphate) (RDP)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Resorcinol bis (Diphenyl Phosphate) (RDP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: C30H24O8P2Cas No.: 57583-54-7RDP is a halogen-free phosphorus-based flame retardant.Use:RDP flame retardant provides a halogen-free solution for flame retarding PC/ABS, PPO/HIPS and other polymers.Storage: RDP can be stored in containers made of carbon steel lined with epoxy resin or made of stainless steel away from incompatible materials.Safety and Handling: If it becomes in contact with the eyes, wash with a large amount of water for at least 15 minutes. If it becomes in contact with the skin, wash with cold water or soap water. Appropriate ventilations is required where there is a chance of exposure. Excess exposure to the product should be avoided.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.32 g/cc

@Temperature 25.0 °C
1.30 - 1.32 g/cc

@Temperature 77.0 °F
Viscosity 400 - 800 cP

@Temperature 25.0 °C
400 - 800 cP

@Temperature 77.0 °F
cPs
Component Elements Properties Metric English Comments
Phosphorous, P <= 10.9 %
<= 10.9 %
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Acidity <0.1
mg KOH/g
CAS Number 57583-54-7
Color (APHA) < 100
Molecular Formula C30H24O8P2
Phenol (ppm) < 200
TGA (°C) 320
5% weight loss, TA instruments, model 2950, 10°C/min under N<sub>2</sub>
360
10% weight loss, TA instruments, model 2950, 10°C/min under N<sub>2</sub>
410
50% weight loss, TA instruments, model 2950, 10°C/min under N<sub>2</sub>
TPP (%) < 3.5