Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oceanchem Group Zinc Bromide

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Zinc Bromide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: ZnBr2Cas No.: 7699-45-8Mainly applied in ocean oil wells as complete liquid, stationary liquid and amend liquid.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Density 2.30 g/cc

@Temperature 20.0 °C
0.0831 lb/in³

@Temperature 68.0 °F
liquid
pH 3.0 - 6.0
3.0 - 6.0
liquid
Component Elements Properties Metric English Comments
Lead, Pb 0.0010 %
0.0010 %
Solid
0.0010 %
0.0010 %
Liquid
Descriptive Properties Value Comments
Appearance Colorless transparent liquid
Liquid
White granular powder
Solid
Bromate Non-reaction
Solid
Non-reaction
Liquid
CAS Number 7699-45-8
Chloride (%) <0.5
Liquid
<1.0
Solid
Content (%) >70
Liquid
>96
Solid
Insoluble (%) <0.3
Solid
<0.3
Liquid
Molecular Formula ZnBr2
Sulphate (%) <0.01
Liquid
<0.02
Solid
Copyright © lookpolymers.com All Rights Reserved