Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Omni Plastics OmniTech™ CPP XE72-A BK17 ESD Polypropylene Conductive

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Omni Plastics
Trade Name OmniTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniTech™ CPP XE72-A BK17 ESD Polypropylene Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and Improved Optical Clarity.Applications:flame retardant storage containers, static dissipative trays, internally lubricated gears and rollers, and NSF compliant pool and filler components. Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Electrical Properties Metric English Comments
Surface Resistance 1000 ohm - 1e+05
1000 ohm - 1e+05
1 volt; ASTM D4496
10000 - 1.00e+6 ohm
10000 - 1.00e+6 ohm
10 volts; ASTM D4496