Omni Plastics OmniTech™ PA6/6 SI2 FD Wear-and-Friction Silicone filled Nylon

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Omni Plastics
Trade Name OmniTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniTech™ PA6/6 SI2 FD Wear-and-Friction Silicone filled Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and Improved Optical Clarity.Applications:flame retardant storage containers, static dissipative trays, internally lubricated gears and rollers, and NSF compliant pool and filler components. Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ASTM D638
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.347 J/cm
0.650 ft-lb/in
ASTM D256