Al-50%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 138 MPa
20000 psi
Tensile Strength, Yield 125 MPa
18100 psi
Modulus of Elasticity 109 GPa
15800 ksi
Flexural Strength 172 MPa
24900 psi
Three Point Bend
Thermal Properties Metric English Comments
CTE, linear 9.20 µm/m-°C

@Temperature -173 - 27.0 °C
5.11 µin/in-°F

@Temperature -279 - 80.6 °F
10.3 µm/m-°C

@Temperature 25.0 - 100 °C
5.72 µin/in-°F

@Temperature 77.0 - 212 °F
12.7 µm/m-°C

@Temperature 25.0 - 200 °C
7.06 µin/in-°F

@Temperature 77.0 - 392 °F
13.1 µm/m-°C

@Temperature 25.0 - 300 °C
7.28 µin/in-°F

@Temperature 77.0 - 572 °F
14.4 µm/m-°C

@Temperature 25.0 - 500 °C
8.00 µin/in-°F

@Temperature 77.0 - 932 °F
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Thermal Conductivity 122 W/m-K

@Temperature 200 °C
847 BTU-in/hr-ft²-°F

@Temperature 392 °F
149 W/m-K

@Temperature 25.0 °C
1030 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Component Elements Properties Metric English Comments
Aluminum, Al 50 %
50 %
Silicon, Si 50 %
50 %
Users viewing this material also viewed the following: