Material Notes:
Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.
Physical Properties Metric English Comments
Density 7.90 g/cc
0.285 lb/in³
RT
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 800 MPa
116000 psi
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
Tensile Strength, Yield 250 MPa

@Strain 0.200 %
36300 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
300 MPa

@Strain 0.200 %
43500 psi

@Strain 0.200 %
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1
330 MPa

@Strain 1.00 %
47900 psi

@Strain 1.00 %
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1
190 MPa

@Strain 0.200 %,
Temperature 200 °C
27600 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
210 MPa

@Strain 0.200 %,
Temperature 100 °C
30500 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 50 %
50 %
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
Modulus of Elasticity 200 GPa
29000 ksi
RT
172 GPa

@Temperature 400 °C
24900 ksi

@Temperature 752 °F
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 100 °C
8.89 µin/in-°F

@Temperature 212 °F
18.0 µm/m-°C

@Temperature 400 °C
10.0 µin/in-°F

@Temperature 752 °F
Specific Heat Capacity 0.500 J/g-°C
0.120 BTU/lb-°F
RT
Thermal Conductivity 15.0 W/m-K
104 BTU-in/hr-ft²-°F
RT
20.0 W/m-K

@Temperature 400 °C
139 BTU-in/hr-ft²-°F

@Temperature 752 °F
Component Elements Properties Metric English Comments
Carbon, C 0.10 %
0.10 %
Chromium, Cr 17 %
17 %
Iron, Fe 75.9 %
75.9 %
Nickel, Ni 7.0 %
7.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000730 ohm-cm
0.0000730 ohm-cm
RT