Outokumpu 4550 Austenitic Stainless Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel
Manufacturer Outokumpu
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Outokumpu 4550 Austenitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto) and rod forms.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 595 MPa
86300 psi
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield 200 MPa

@Strain 0.200 %
29000 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
260 MPa

@Strain 0.200 %
37700 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
290 MPa

@Strain 1.00 %
42100 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
125 MPa

@Strain 0.200 %,
Temperature 400 °C
18100 psi

@Strain 0.200 %,
Temperature 752 °F
EN min.; EN 10002-5
157 MPa

@Strain 0.200 %,
Temperature 200 °C
22800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
176 MPa

@Strain 0.200 %,
Temperature 100 °C
25500 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 45 %
45 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Component Elements Properties Metric English Comments
Carbon, C 0.050 %
0.050 %
Chromium, Cr 17.5 %
17.5 %
Iron, Fe 72.91 %
72.91 %
Nickel, Ni 9.5 %
9.5 %
Nitrogen, N 0.040 %
0.040 %