Ovation Polymers Nemcon™ E HDPE 11000 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ E HDPE 11000 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HDPE-ESD Range Conductivity with improved processability and UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.0 MPa
3340 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ASTM D638
Elongation at Break 12 - 15 %
12 - 15 %
50 mm/min; ASTM D638
Tensile Modulus 0.820 GPa
119 ksi
50 mm/min; ASTM D638
Flexural Strength 23.0 MPa
3340 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 0.510 GPa
74.0 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C

@Thickness 3.20 mm
122 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 3000 ohm
3000 ohm
ASTM D257