Material Notes:
Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Linear Mold Shrinkage 0.00 - 0.0020 cm/cm

@Thickness 3.17 mm
0.00 - 0.0020 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.00 - 0.0020 cm/cm

@Thickness 3.17 mm
0.00 - 0.0020 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 168 MPa
24400 psi
50 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
50 mm/min; ASTM D638
Tensile Modulus 10.8 GPa
1570 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 240 MPa
34800 psi
1.3 mm/min; ASTM D790
Flexural Modulus 13.5 GPa
1960 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 250 - 258 °C
482 - 496 °F
DSC @ 15°C / min; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 220 °C

@Thickness 3.20 mm
428 °F

@Thickness 0.126 in
unannealed; ASTM D648