Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for ASA/AES, Unreinforced, Extruded/Molded

Category Polymer , Thermoplastic , AES Polymer , ASA Polymer , ASA/AES, Unreinforced, Extruded/Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for ASA/AES, Unreinforced, Extruded/Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "ASA/AES, Unreinforced, Extruded/Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.530 - 0.530 J/cm

@Temperature -40.0 - -40.0 °C
0.993 - 0.993 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.530 J/cm Grade Count:1
0.530 - 0.530 J/cm

@Thickness 3.17 - 3.17 mm
0.993 - 0.993 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.530 J/cm Grade Count:1