Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.882 - 3.50 g/cc
0.0319 - 0.126 lb/in³
Average value: 1.06 g/cc Grade Count:387
Water Absorption 0.0250 - 2.30 %
0.0250 - 2.30 %
Average value: 0.421 % Grade Count:74
Moisture Absorption at Equilibrium 0.150 - 0.220 %
0.150 - 0.220 %
Average value: 0.200 % Grade Count:23
Water Absorption at Saturation 0.300 - 1.03 %
0.300 - 1.03 %
Average value: 0.734 % Grade Count:20
Viscosity 255000 - 255000 cP

@Temperature 240 - 240 °C
255000 - 255000 cP

@Temperature 464 - 464 °F
Average value: 255000 cP Grade Count:1
Maximum Moisture Content 0.0100 - 0.150
0.0100 - 0.150
Average value: 0.0374 Grade Count:46
Linear Mold Shrinkage 0.00150 - 0.00800 cm/cm
0.00150 - 0.00800 in/in
Average value: 0.00526 cm/cm Grade Count:248
Linear Mold Shrinkage, Transverse 0.00250 - 0.00900 cm/cm
0.00250 - 0.00900 in/in
Average value: 0.00541 cm/cm Grade Count:22
Melt Flow 0.0800 - 80.0 g/10 min
0.0800 - 80.0 g/10 min
Average value: 14.7 g/10 min Grade Count:399
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90.0 - 119
90.0 - 119
Average value: 107 Grade Count:221
Hardness, H358/30 85.0 - 104 MPa
12300 - 15100 psi
Average value: 93.1 MPa Grade Count:9
Ball Indentation Hardness 80.0 - 120 MPa
11600 - 17400 psi
Average value: 99.3 MPa Grade Count:26
Tensile Strength, Ultimate 24.1 - 73.1 MPa
3500 - 10600 psi
Average value: 38.5 MPa Grade Count:150
20.0 - 52.0 MPa

@Temperature -18.0 - 90.0 °C
2900 - 7540 psi

@Temperature -0.400 - 194 °F
Average value: 35.8 MPa Grade Count:3
Tensile Strength, Yield 20.0 - 73.1 MPa
2900 - 10600 psi
Average value: 43.4 MPa Grade Count:339
64.0 - 64.0 MPa

@Temperature -18.0 - -18.0 °C
9280 - 9280 psi

@Temperature -0.400 - -0.400 °F
Average value: 64.0 MPa Grade Count:1
Elongation at Break 1.40 - 110 %
1.40 - 110 %
Average value: 24.9 % Grade Count:244
15.0 - 15.0 %

@Temperature -18.0 - -18.0 °C
15.0 - 15.0 %

@Temperature -0.400 - -0.400 °F
Average value: 15.0 % Grade Count:1
Elongation at Yield 1.70 - 20.0 %
1.70 - 20.0 %
Average value: 3.39 % Grade Count:130
Modulus of Elasticity 0.778 - 6.10 GPa
113 - 885 ksi
Average value: 2.30 GPa Grade Count:220
2.81 - 2.81 GPa

@Temperature -18.0 - -18.0 °C
408 - 408 ksi

@Temperature -0.400 - -0.400 °F
Average value: 2.81 GPa Grade Count:1
Flexural Yield Strength 10.3 - 111 MPa
1500 - 16100 psi
Average value: 67.6 MPa Grade Count:258
Flexural Modulus 0.0241 - 6.89 GPa
3.50 - 1000 ksi
Average value: 2.34 GPa Grade Count:305
1.50 - 4.00 GPa

@Temperature 60.0 - 90.0 °C
218 - 580 ksi

@Temperature 140 - 194 °F
Average value: 2.84 GPa Grade Count:2
Izod Impact, Notched 0.100 - 6.40 J/cm
0.187 - 12.0 ft-lb/in
Average value: 2.22 J/cm Grade Count:309
0.350 - 3.00 J/cm

@Temperature -50.0 - 0.000 °C
0.656 - 5.62 ft-lb/in

@Temperature -58.0 - 32.0 °F
Average value: 0.922 J/cm Grade Count:13
0.480 - 1.87 J/cm

@Temperature -40.0 - 0.000 °C
0.899 - 3.50 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.922 J/cm Grade Count:8
0.480 - 1.87 J/cm

@Thickness 3.17 - 3.20 mm
0.899 - 3.50 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 0.922 J/cm Grade Count:8
Izod Impact, Unnotched 0.981 J/cm - NB
1.84 ft-lb/in - NB
Average value: 7.89 J/cm Grade Count:12
0.392266 - 2.54973 J/cm

@Temperature -30.0 - -20.0 °C
0.734875 - 4.77669 ft-lb/in

@Temperature -22.0 - -4.00 °F
Average value: 0.848 J/cm Grade Count:27
0.392266 - 2.54973 J/cm

@Thickness 3.20 - 6.40 mm
0.734875 - 4.77669 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.848 J/cm Grade Count:27
Izod Impact, Notched (ISO) 2.00 - 48.0 kJ/m²
0.952 - 22.8 ft-lb/in²
Average value: 18.1 kJ/m² Grade Count:79
4.00 - 16.0 kJ/m²

@Temperature -30.0 - -18.0 °C
1.90 - 7.61 ft-lb/in²

@Temperature -22.0 - -0.400 °F
Average value: 8.77 kJ/m² Grade Count:39
6.00 - 13.0 kJ/m²

@Temperature -40.0 - -20.0 °C
2.86 - 6.19 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 8.77 kJ/m² Grade Count:3
6.00 - 13.0 kJ/m²

@Thickness 4.00 - 4.00 mm
2.86 - 6.19 ft-lb/in²

@Thickness 0.157 - 0.157 in
Average value: 8.77 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 39.2 kJ/m² - NB
18.7 ft-lb/in² - NB
Average value: 87.4 kJ/m² Grade Count:25
60.0 - 70.0 kJ/m²

@Temperature -30.0 - -30.0 °C
28.6 - 33.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 68.0 kJ/m² Grade Count:5
NB - NB

@Temperature -20.0 - -20.0 °C
NB - NB

@Temperature -4.00 - -4.00 °F
Average value: 68.0 kJ/m² Grade Count:1
NB - NB

@Thickness 4.00 - 4.00 mm
NB - NB

@Thickness 0.157 - 0.157 in
Average value: 68.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.00 J/cm² - NB
9.52 ft-lb/in² - NB
Average value: 11.6 J/cm² Grade Count:90
0.300 J/cm² - NB

@Temperature -40.0 - -20.0 °C
1.43 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 6.53 J/cm² Grade Count:61
Charpy Impact, Notched 0.500 - 14.0 J/cm²
2.38 - 66.6 ft-lb/in²
Average value: 1.91 J/cm² Grade Count:120
0.300 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.789 J/cm² Grade Count:60
Gardner Impact 1.80 - 22.6 J
1.33 - 16.7 ft-lb
Average value: 16.7 J Grade Count:6
Falling Dart Impact 2.82 - 37.6 J
2.08 - 27.7 ft-lb
Average value: 22.7 J Grade Count:6
Tensile Creep Modulus, 1 hour 2200 - 2500 MPa
319000 - 363000 psi
Average value: 2370 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 1500 - 1900 MPa
218000 - 276000 psi
Average value: 1770 MPa Grade Count:3
Taber Abrasion, mg/1000 Cycles 50.0 - 115
50.0 - 115
Average value: 101 Grade Count:9
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 - 1.00e+18 ohm-cm
1.00e+9 - 1.00e+18 ohm-cm
Average value: 1.28e+16 ohm-cm Grade Count:96
Surface Resistance 1000 - 2.00e+17 ohm
1000 - 2.00e+17 ohm
Average value: 9.22e+15 ohm Grade Count:70
Static Decay 0.300 - 3.00 sec
0.300 - 3.00 sec
Average value: 1.56 sec Grade Count:5
Dielectric Constant 2.60 - 3.50
2.60 - 3.50
Average value: 2.93 Grade Count:46
Dielectric Strength 15.7 - 53.0 kV/mm
400 - 1350 kV/in
Average value: 30.0 kV/mm Grade Count:75
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved