This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.700 - 1.56 g/cc
0.0253 - 0.0564 lb/in³
Average value: 1.43 g/cc Grade Count:19
Viscosity Test 72.0 - 94.0 cm³/g
72.0 - 94.0 cm³/g
Average value: 79.3 cm³/g Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111 - 119
111 - 119
Average value: 116 Grade Count:10
Hardness, Shore D 80.0 - 84.0
80.0 - 84.0
Average value: 82.9 Grade Count:7
Tensile Strength, Yield 48.4 - 58.0 MPa
7020 - 8410 psi
Average value: 53.5 MPa Grade Count:15
Elongation at Break 12.0 - 163 %
12.0 - 163 %
Average value: 53.5 % Grade Count:6
Elongation at Yield 4.00 - 7.00 %
4.00 - 7.00 %
Average value: 5.50 % Grade Count:4
Modulus of Elasticity 1.79 - 3.10 GPa
260 - 450 ksi
Average value: 2.68 GPa Grade Count:16
Flexural Yield Strength 46.2 - 108 MPa
6700 - 15700 psi
Average value: 88.8 MPa Grade Count:13
Flexural Modulus 2.26 - 3.50 GPa
328 - 508 ksi
Average value: 2.85 GPa Grade Count:13
Izod Impact, Notched 0.960 - 4.80 J/cm
1.80 - 8.99 ft-lb/in
Average value: 1.95 J/cm Grade Count:13
Izod Impact, Notched (ISO) 2.31 - 2.31 kJ/m²

@Temperature 0.000 - 0.000 °C
1.10 - 1.10 ft-lb/in²

@Temperature 32.0 - 32.0 °F
Average value: 2.31 kJ/m² Grade Count:1
2.31 - 2.31 kJ/m²

@Thickness 3.18 - 3.18 mm
1.10 - 1.10 ft-lb/in²

@Thickness 0.125 - 0.125 in
Average value: 2.31 kJ/m² Grade Count:1
Charpy Impact Unnotched NB
NB
Grade Count:4
Charpy Impact, Notched 1.00 - 1.36 J/cm²
4.76 - 6.47 ft-lb/in²
Average value: 1.11 J/cm² Grade Count:4
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 46.7 - 115 °C
116 - 239 °F
Average value: 100 °C Grade Count:17
Vicat Softening Point 98.0 - 115 °C
208 - 239 °F
Average value: 109 °C Grade Count:5
Flammability, UL94 V-0
V-0
Grade Count:8
Oxygen Index 56.0 - 75.0 %
56.0 - 75.0 %
Average value: 68.5 % Grade Count:5
Processing Properties Metric English Comments
Melt Temperature 191 - 210 °C
376 - 410 °F
Average value: 203 °C Grade Count:11