Overview of materials for Ethylene Acrylic Acid

Category Polymer , Thermoplastic , Ethylene Acrylic Acid
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Ethylene Acrylic Acid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.910 - 1.27 g/cc
0.0329 - 0.0459 lb/in³
Average value: 0.949 g/cc Grade Count:65
Water Absorption 0.0500 %
0.0500 %
Average value: 0.0500 % Grade Count:5
Moisture Absorption at Equilibrium 0.0500 %
0.0500 %
Average value: 0.0500 % Grade Count:5
pH 2.00 - 12.0
2.00 - 12.0
Average value: 7.91 Grade Count:9
Viscosity 50.0 - 4000 cP
50.0 - 4000 cP
Average value: 578 cP Grade Count:9
575 - 30000 cP

@Temperature 140 - 190 °C
575 - 30000 cP

@Temperature 284 - 374 °F
Average value: 5530 cP Grade Count:12
Methyl Acrylate Content 6.50 - 20.0 %
6.50 - 20.0 %
Average value: 12.8 % Grade Count:8
Acrylic Acid Content 6.00 - 15.0 %
6.00 - 15.0 %
Average value: 7.90 % Grade Count:15
Thickness 60.0 microns
2.36 mil
Average value: 60.0 microns Grade Count:4
Melt Flow 0.500 - 1300 g/10 min
0.500 - 1300 g/10 min
Average value: 60.8 g/10 min Grade Count:49
Mechanical Properties Metric English Comments
Hardness, Shore A 62.0 - 85.0
62.0 - 85.0
Average value: 73.3 Grade Count:4
Hardness, Shore D 22.0 - 50.0
22.0 - 50.0
Average value: 40.2 Grade Count:6
Tensile Strength, Ultimate 1.50 - 24.7 MPa
218 - 3580 psi
Average value: 14.9 MPa Grade Count:25
Film Tensile Strength at Yield, MD 8.10 - 9.40 MPa
1170 - 1360 psi
Average value: 8.68 MPa Grade Count:4
Film Tensile Strength at Yield, TD 7.90 - 9.20 MPa
1150 - 1330 psi
Average value: 8.32 MPa Grade Count:4
Tensile Strength, Yield 4.00 - 10.8 MPa
580 - 1570 psi
Average value: 7.34 MPa Grade Count:21
Film Elongation at Break, MD 210 - 540 %
210 - 540 %
Average value: 433 % Grade Count:11
Film Elongation at Break, TD 440 - 750 %
440 - 750 %
Average value: 567 % Grade Count:11
Elongation at Break 50.0 - 800 %
50.0 - 800 %
Average value: 371 % Grade Count:29
Modulus of Elasticity 0.0221 - 0.124 GPa
3.21 - 18.0 ksi
Average value: 0.0758 GPa Grade Count:15
Flexural Modulus 0.00500 - 0.0427 GPa
0.725 - 6.20 ksi
Average value: 0.0222 GPa Grade Count:5
Secant Modulus, MD 0.0278 - 0.170 GPa
4.03 - 24.7 ksi
Average value: 0.101 GPa Grade Count:7
Secant Modulus, TD 0.0271 - 0.175 GPa
3.93 - 25.4 ksi
Average value: 0.0967 GPa Grade Count:7
Tensile Impact Strength 25.0 - 25.0 kJ/m²

@Temperature -40.0 - -40.0 °C
11.9 - 11.9 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 25.0 kJ/m² Grade Count:1
Elmendorf Tear Strength MD 255 - 450 g
255 - 450 g
Average value: 346 g Grade Count:4
Elmendorf Tear Strength TD 305 - 510 g
305 - 510 g
Average value: 429 g Grade Count:4
Elmendorf Tear Strength, MD 1.31 - 8.93 g/micron
33.3 - 227 g/mil
Average value: 5.27 g/micron Grade Count:11
Elmendorf Tear Strength, TD 5.10 - 30.2 g/micron
130 - 767 g/mil
Average value: 11.0 g/micron Grade Count:11
Dart Drop 6.56 - 11.8 g/micron
167 - 300 g/mil
Average value: 8.00 g/micron Grade Count:8
Dart Drop Test 4.30 - 7.90 g
0.00948 - 0.0174 lb
Average value: 5.50 g Grade Count:3
Seal Strength 1800 - 2500 g/25 mm
1800 - 2500 g/in
Average value: 2080 g/25 mm Grade Count:4
Film Tensile Strength at Break, MD 20.7 - 42.7 MPa
3000 - 6190 psi
Average value: 30.6 MPa Grade Count:11
Film Tensile Strength at Break, TD 22.1 - 44.8 MPa
3200 - 6500 psi
Average value: 30.3 MPa Grade Count:11
Thermal Properties Metric English Comments
Melting Point 66.7 - 216 °C
152 - 421 °F
Average value: 108 °C Grade Count:43
Vicat Softening Point 38.3 - 92.2 °C
101 - 198 °F
Average value: 68.0 °C Grade Count:39
Dropping Point 76.0 - 105 °C
169 - 221 °F
Average value: 95.1 °C Grade Count:12
Optical Properties Metric English Comments
Haze 3.00 - 18.3 %
3.00 - 18.3 %
Average value: 7.20 % Grade Count:8
Gloss 39.0 - 100 %
39.0 - 100 %
Average value: 62.5 % Grade Count:8
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Average value: 1.00e+15 ohm-cm Grade Count:9
Dielectric Constant 2.30 - 2.80
2.30 - 2.80
Average value: 2.48 Grade Count:5
Dissipation Factor 0.00700 - 0.0130
0.00700 - 0.0130
Average value: 0.0102 Grade Count:5
Chemical Properties Metric English Comments
Total Acid Number 0.000 - 200
0.000 - 200
Average value: 67.4 Grade Count:8
Processing Properties Metric English Comments
Processing Temperature 191 - 310 °C
376 - 590 °F
Average value: 262 °C Grade Count:13
Nozzle Temperature 177 - 290 °C
351 - 554 °F
Average value: 225 °C Grade Count:5
Adapter Temperature 180 - 300 °C
356 - 572 °F
Average value: 229 °C Grade Count:8
Die Temperature 170 - 300 °C
338 - 572 °F
Average value: 228 °C Grade Count:11
Melt Temperature 135 - 305 °C
275 - 581 °F
Average value: 211 °C Grade Count:16