Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Carbon Black Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.940 - 0.956 g/cc
0.0340 - 0.0345 lb/in³
Average value: 0.950 g/cc Grade Count:8
Environmental Stress Crack Resistance 400 - 5000 hour
400 - 5000 hour
Average value: 3170 hour Grade Count:6
Melt Flow 0.265 - 34.0 g/10 min
0.265 - 34.0 g/10 min
Average value: 9.85 g/10 min Grade Count:9
Mechanical Properties Metric English Comments
Hardness, Shore D 59.0 - 68.0
59.0 - 68.0
Average value: 64.3 Grade Count:7
Tensile Strength, Ultimate 22.0 - 31.0 MPa
3190 - 4500 psi
Average value: 28.3 MPa Grade Count:6
Tensile Strength, Yield 17.5 - 23.4 MPa
2540 - 3390 psi
Average value: 21.2 MPa Grade Count:7
Elongation at Break 600 - 800 %
600 - 800 %
Average value: 771 % Grade Count:7
Flexural Modulus 0.580 - 0.830 GPa
84.1 - 120 ksi
Average value: 0.760 GPa Grade Count:6
Izod Impact, Notched 3.20 - 7.50 J/cm
5.99 - 14.1 ft-lb/in
Average value: 4.64 J/cm Grade Count:5
Thermal Properties Metric English Comments
Vicat Softening Point 115 - 129 °C
239 - 264 °F
Average value: 124 °C Grade Count:6
Brittleness Temperature -118 - -70.0 °C
-180 - -94.0 °F
Average value: -86.6 °C Grade Count:7