Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Ionomer, Molded

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Ionomer, Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.940 - 0.970 g/cc
0.0340 - 0.0350 lb/in³
Average value: 0.957 g/cc Grade Count:48
Linear Mold Shrinkage 0.00600 - 0.0180 cm/cm
0.00600 - 0.0180 in/in
Average value: 0.0100 cm/cm Grade Count:9
Melt Flow 0.700 - 20.0 g/10 min
0.700 - 20.0 g/10 min
Average value: 2.83 g/10 min Grade Count:46
Mechanical Properties Metric English Comments
Hardness, Shore D 30.0 - 68.0
30.0 - 68.0
Average value: 58.5 Grade Count:41
Tensile Strength, Ultimate 12.0 - 37.2 MPa
1740 - 5400 psi
Average value: 25.7 MPa Grade Count:47
Tensile Strength, Yield 3.10 - 21.0 MPa
450 - 3050 psi
Average value: 14.0 MPa Grade Count:25
Elongation at Break 225 - 680 %
225 - 680 %
Average value: 414 % Grade Count:48
Flexural Modulus 0.0296 - 0.758 GPa
4.29 - 110 ksi
Average value: 0.308 GPa Grade Count:48
Izod Impact, Notched 3.65 J/cm - NB
6.84 ft-lb/in - NB
Average value: 6.58 J/cm Grade Count:20
8.5424 - 8.5424 J/cm

@Temperature -30.0 - -30.0 °C
16.003 - 16.003 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 8.54 J/cm Grade Count:5
Izod Impact, Notched (ISO) NB
NB
Grade Count:4
Gardner Impact 36.1552 - 36.1552 J

@Temperature -30.0 - -30.0 °C
26.6667 - 26.6667 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 36.2 J Grade Count:5
Tensile Impact Strength 340 - 1320 kJ/m²
162 - 628 ft-lb/in²
Average value: 837 kJ/m² Grade Count:27
Tear Strength 102 - 164 kN/m
582 - 935 pli
Average value: 136 kN/m Grade Count:6
Thermal Properties Metric English Comments
CTE, linear 76.0 - 170 µm/m-°C
42.2 - 94.4 µin/in-°F
Average value: 130 µm/m-°C Grade Count:20
Thermal Conductivity 0.230 - 0.250 W/m-K
1.60 - 1.74 BTU-in/hr-ft²-°F
Average value: 0.244 W/m-K Grade Count:15
Melting Point 47.0 - 105 °C
117 - 221 °F
Average value: 84.7 °C Grade Count:40
Deflection Temperature at 0.46 MPa (66 psi) 34.0 - 80.0 °C
93.2 - 176 °F
Average value: 45.3 °C Grade Count:24
Vicat Softening Point 40.0 - 74.0 °C
104 - 165 °F
Average value: 60.4 °C Grade Count:39
Brittleness Temperature -112 - -71.0 °C
-170 - -95.8 °F
Average value: -98.0 °C Grade Count:12
Flame Spread 17.8 - 27.9 mm/min
0.701 - 1.10 in/min
Average value: 23.4 mm/min Grade Count:15
Optical Properties Metric English Comments
Haze 4.00 - 27.0 %
4.00 - 27.0 %
Average value: 10.9 % Grade Count:18
Gloss 25.0 - 143 %
25.0 - 143 %
Average value: 60.3 % Grade Count:12
Transmission, Visible 90.0 %
90.0 %
Average value: 90.0 % Grade Count:6
Processing Properties Metric English Comments
Nozzle Temperature 238 - 271 °C
460 - 520 °F
Average value: 254 °C Grade Count:5
Melt Temperature 238 - 288 °C
460 - 550 °F
Average value: 263 °C Grade Count:5
Mold Temperature 15.6 - 60.0 °C
60.0 - 140 °F
Average value: 37.8 °C Grade Count:5
Drying Temperature 60.0 - 79.4 °C
140 - 175 °F
Average value: 69.7 °C Grade Count:5
Moisture Content 0.0800 %
0.0800 %
Average value: 0.0800 % Grade Count:5
Users viewing this material also viewed the following: