Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Liquid Crystal Polymer (LCP), Carbon Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.39 - 1.61 g/cc
0.0502 - 0.0582 lb/in³
Average value: 1.50 g/cc Grade Count:17
Filler Content 10.0 - 40.0 %
10.0 - 40.0 %
Average value: 27.7 % Grade Count:13
Water Absorption 0.0350 - 0.100 %
0.0350 - 0.100 %
Average value: 0.0783 % Grade Count:3
Linear Mold Shrinkage 0.000100 - 0.00200 cm/cm
0.000100 - 0.00200 in/in
Average value: 0.000593 cm/cm Grade Count:15
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 102 - 200 MPa
14800 - 29000 psi
Average value: 148 MPa Grade Count:17
Elongation at Break 0.250 - 4.00 %
0.250 - 4.00 %
Average value: 1.36 % Grade Count:15
Modulus of Elasticity 13.8 - 36.2 GPa
2000 - 5250 ksi
Average value: 27.5 GPa Grade Count:15
Flexural Yield Strength 155 - 290 MPa
22500 - 42000 psi
Average value: 214 MPa Grade Count:15
Flexural Modulus 11.7 - 31.0 GPa
1700 - 4500 ksi
Average value: 22.6 GPa Grade Count:17
Izod Impact, Notched 0.427 - 3.20 J/cm
0.800 - 6.00 ft-lb/in
Average value: 0.931 J/cm Grade Count:15
Izod Impact, Unnotched 2.14 - 8.54 J/cm
4.00 - 16.0 ft-lb/in
Average value: 4.14 J/cm Grade Count:14
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 216 - 318 °C
420 - 605 °F
Average value: 266 °C Grade Count:16
Flammability, UL94 V-0
V-0
Grade Count:9
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 1.00e+8 ohm-cm
1.00 - 1.00e+8 ohm-cm
Average value: 2.00e+7 ohm-cm Grade Count:8
Processing Properties Metric English Comments
Melt Temperature 271 - 399 °C
520 - 750 °F
Average value: 337 °C Grade Count:13
Mold Temperature 37.8 - 121 °C
100 - 250 °F
Average value: 83.1 °C Grade Count:15
Drying Temperature 149 - 163 °C
300 - 325 °F
Average value: 149 °C Grade Count:13
Dew Point -28.9 °C
-20.0 °F
Average value: -28.9 °C Grade Count:8
Injection Pressure 34.5 - 124 MPa
5000 - 18000 psi
Average value: 88.2 MPa Grade Count:14