Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Medium Density Polyethylene (MDPE), Extruded

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Medium Density Polyethylene (MDPE), Extruded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.930 - 1.05 g/cc
0.0336 - 0.0379 lb/in³
Average value: 0.945 g/cc Grade Count:22
Environmental Stress Crack Resistance 1000 - 5000 hour
1000 - 5000 hour
Average value: 2290 hour Grade Count:10
>= 2000 hour

@Temperature 80.0 - 80.0 °C
>= 2000 hour

@Temperature 176 - 176 °F
Average value: 2000 hour Grade Count:2
Melt Flow 0.200 - 21.0 g/10 min
0.200 - 21.0 g/10 min
Average value: 3.84 g/10 min Grade Count:22
Mechanical Properties Metric English Comments
Hardness, Shore D 48.0 - 69.0
48.0 - 69.0
Average value: 57.2 Grade Count:11
Tensile Strength, Ultimate 12.5 - 33.1 MPa
1810 - 4800 psi
Average value: 22.8 MPa Grade Count:5
Tensile Strength, Yield 13.8 - 31.0 MPa
2000 - 4500 psi
Average value: 19.7 MPa Grade Count:16
Elongation at Break 50.0 - 1000 %
50.0 - 1000 %
Average value: 510 % Grade Count:17
Modulus of Elasticity 0.800 GPa
116 ksi
Average value: 0.800 GPa Grade Count:3
Flexural Modulus 0.590 - 0.840 GPa
85.6 - 122 ksi
Average value: 0.694 GPa Grade Count:9
Thermal Properties Metric English Comments
Melting Point 126 - 128 °C
259 - 262 °F
Average value: 126 °C Grade Count:5
Vicat Softening Point 114 - 127 °C
237 - 261 °F
Average value: 119 °C Grade Count:4
Brittleness Temperature -100 - -70.0 °C
-148 - -94.0 °F
Average value: -79.3 °C Grade Count:8
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 - 3.00e+16 ohm-cm
1.00e+15 - 3.00e+16 ohm-cm
Average value: 1.16e+16 ohm-cm Grade Count:7
Dielectric Constant 2.30 - 2.55
2.30 - 2.55
Average value: 2.38 Grade Count:3
Dielectric Strength 21.7 - 39.4 kV/mm
550 - 1000 kV/in
Average value: 29.2 kV/mm Grade Count:6
Dissipation Factor 0.000500
0.000500
Average value: 0.000500 Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 180 - 240 °C
356 - 464 °F
Average value: 210 °C Grade Count:6
Die Temperature 185 - 218 °C
365 - 425 °F
Average value: 198 °C Grade Count:7
Melt Temperature 160 - 230 °C
320 - 446 °F
Average value: 190 °C Grade Count:8
Head Temperature 185 - 210 °C
365 - 410 °F
Average value: 196 °C Grade Count:6
Copyright © lookpolymers.com All Rights Reserved