Overview of materials for Methacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Methacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.500 - 1.20 g/cc
0.0181 - 0.0434 lb/in³
Average value: 1.03 g/cc Grade Count:48
Viscosity 12.0 - 950000 cP
12.0 - 950000 cP
Average value: 118000 cP Grade Count:64
Mechanical Properties Metric English Comments
Hardness, Shore D 60.0 - 70.0
60.0 - 70.0
Average value: 64.4 Grade Count:8
Tensile Strength, Ultimate 7.60 - 31.0 MPa
1100 - 4500 psi
Average value: 17.1 MPa Grade Count:30
0.0965266 - 0.0965266 MPa

@Temperature 18.3 - 149 °C
14.0000 - 14.0000 psi

@Temperature 65.0 - 300 °F
Average value: 0.0965 MPa Grade Count:1
Elongation at Break 5.00 - 180 %
5.00 - 180 %
Average value: 77.1 % Grade Count:39
Elongation at Yield 15.0 - 70.0 %
15.0 - 70.0 %
Average value: 36.3 % Grade Count:8
Modulus of Elasticity 0.0689 - 1.90 GPa
10.0 - 275 ksi
Average value: 0.579 GPa Grade Count:25
Shear Strength 1.00 - 32.0 MPa
145 - 4640 psi
Average value: 11.2 MPa Grade Count:44
Adhesive Bond Strength 0.600 - 29.0 MPa
87.0 - 4200 psi
Average value: 19.5 MPa Grade Count:23
Tensile Impact Strength 35.7 - 46.2 kJ/m²
17.0 - 22.0 ft-lb/in²
Average value: 41.3 kJ/m² Grade Count:9
Peel Strength 1.75 - 11.4 kN/m
10.0 - 65.0 pli
Average value: 5.00 kN/m Grade Count:18
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
Average value: 0.800 µm/m-°C Grade Count:20
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Average value: 0.300 J/g-°C Grade Count:20
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Average value: 0.100 W/m-K Grade Count:20
Maximum Service Temperature, Air 82.2 - 121 °C
180 - 250 °F
Average value: 118 °C Grade Count:45
Minimum Service Temperature, Air -55.0 - -40.0 °C
-67.0 - -40.0 °F
Average value: -51.7 °C Grade Count:39
Flash Point 10.6 - 82.2 °C
51.0 - 180 °F
Average value: 22.5 °C Grade Count:50
Processing Properties Metric English Comments
Cure Time 1.50 - 1440 min
0.0250 - 24.0 hour
Average value: 372 min Grade Count:32
Pot Life 1.00 - 105 min
1.00 - 105 min
Average value: 23.8 min Grade Count:25
45.0 - 45.0 min

@Temperature 95.0 - 95.0 °C
45.0 - 45.0 min

@Temperature 203 - 203 °F
Average value: 45.0 min Grade Count:1