Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.29 - 1.39 g/cc
0.0466 - 0.0502 lb/in³
Average value: 1.34 g/cc Grade Count:8
Filler Content 35.0 - 43.0 %
35.0 - 43.0 %
Average value: 39.6 % Grade Count:5
Water Absorption 0.140 - 1.50 %
0.140 - 1.50 %
Average value: 0.697 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm
0.00100 - 0.00400 in/in
Average value: 0.00243 cm/cm Grade Count:5
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 114 - 145 MPa
16500 - 21000 psi
Average value: 131 MPa Grade Count:8
Elongation at Break 2.00 - 5.00 %
2.00 - 5.00 %
Average value: 3.50 % Grade Count:8
Modulus of Elasticity 7.58 - 13.3 GPa
1100 - 1930 ksi
Average value: 9.64 GPa Grade Count:8
Flexural Yield Strength 162 - 241 MPa
23500 - 35000 psi
Average value: 195 MPa Grade Count:5
Flexural Modulus 6.21 - 8.28 GPa
900 - 1200 ksi
Average value: 7.58 GPa Grade Count:5
Izod Impact, Notched 1.71 - 3.74 J/cm
3.20 - 7.01 ft-lb/in
Average value: 2.30 J/cm Grade Count:5
Izod Impact, Unnotched 9.08 - 13.3 J/cm
17.0 - 25.0 ft-lb/in
Average value: 10.7 J/cm Grade Count:5
Charpy Impact Unnotched 4.50 - 7.12 J/cm²
21.4 - 33.9 ft-lb/in²
Average value: 6.16 J/cm² Grade Count:3
4.50 - 7.25 J/cm²

@Temperature -30.0 - 30.0 °C
21.4 - 34.5 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 6.21 J/cm² Grade Count:3
Charpy Impact, Notched 1.26 - 1.40 J/cm²
6.00 - 6.66 ft-lb/in²
Average value: 1.31 J/cm² Grade Count:3
1.06 - 1.30 J/cm²

@Temperature -30.0 - 30.0 °C
5.04 - 6.19 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.14 J/cm² Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 20.0 - 32.4 µm/m-°C
11.1 - 18.0 µin/in-°F
Average value: 27.5 µm/m-°C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 135 - 177 °C
275 - 350 °F
Average value: 165 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 125 - 171 °C
257 - 340 °F
Average value: 159 °C Grade Count:4
Flammability, UL94 HB
HB
Grade Count:7
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 - 1.00e+14 ohm-cm
1.00e+12 - 1.00e+14 ohm-cm
Average value: 5.27e+13 ohm-cm Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 216 - 266 °C
420 - 510 °F
Average value: 241 °C Grade Count:3
Mold Temperature 65.6 - 104 °C
150 - 220 °F
Average value: 85.0 °C Grade Count:4
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:4