Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Lubricated + Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.43 - 1.69 g/cc
0.0517 - 0.0611 lb/in³
Average value: 1.53 g/cc Grade Count:13
Water Absorption 0.900 - 2.00 %
0.900 - 2.00 %
Average value: 1.59 % Grade Count:8
Linear Mold Shrinkage 0.00200 - 0.00750 cm/cm
0.00200 - 0.00750 in/in
Average value: 0.00533 cm/cm Grade Count:9
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 110 - 205 MPa
16000 - 29700 psi
Average value: 159 MPa Grade Count:7
Tensile Strength, Yield 82.7 - 179 MPa
12000 - 26000 psi
Average value: 138 MPa Grade Count:6
Elongation at Break 2.70 - 7.00 %
2.70 - 7.00 %
Average value: 4.30 % Grade Count:10
Elongation at Yield 2.00 - 3.00 %
2.00 - 3.00 %
Average value: 2.62 % Grade Count:3
Modulus of Elasticity 4.10 - 11.0 GPa
595 - 1600 ksi
Average value: 8.69 GPa Grade Count:7
Flexural Yield Strength 110 - 279 MPa
16000 - 40500 psi
Average value: 207 MPa Grade Count:9
Flexural Modulus 2.96 - 9.65 GPa
430 - 1400 ksi
Average value: 7.58 GPa Grade Count:11
Izod Impact, Notched 0.641 - 1.92 J/cm
1.20 - 3.60 ft-lb/in
Average value: 1.15 J/cm Grade Count:7
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -40.0 - -40.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 8.00 kJ/m² Grade Count:2
Charpy Impact, Notched 0.700 - 1.50 J/cm²
3.33 - 7.14 ft-lb/in²
Average value: 1.15 J/cm² Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 18.0 - 79.2 µm/m-°C
10.0 - 44.0 µin/in-°F
Average value: 33.0 µm/m-°C Grade Count:7
Melting Point 295 °C
563 °F
Average value: 295 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 274 - 290 °C
525 - 554 °F
Average value: 284 °C Grade Count:10
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:5
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+7 - 1.00e+14 ohm-cm
1.00e+7 - 1.00e+14 ohm-cm
Average value: 4.32e+13 ohm-cm Grade Count:7
Dielectric Strength 23.6 kV/mm
600 kV/in
Average value: 23.6 kV/mm Grade Count:5
Processing Properties Metric English Comments
Processing Temperature 293 - 321 °C
560 - 610 °F
Average value: 309 °C Grade Count:3
Mold Temperature 79.4 - 149 °C
175 - 300 °F
Average value: 125 °C Grade Count:3