Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.938 - 2.56 g/cc
0.0339 - 0.0925 lb/in³
Average value: 1.15 g/cc Grade Count:281
0.960 - 0.960 g/cc

@Temperature 290 - 290 °C
0.0347 - 0.0347 lb/in³

@Temperature 554 - 554 °F
Average value: 0.960 g/cc Grade Count:1
Filler Content 15.0 - 60.0 %
15.0 - 60.0 %
Average value: 36.7 % Grade Count:6
Water Absorption 0.0600 - 9.50 %
0.0600 - 9.50 %
Average value: 2.43 % Grade Count:154
Moisture Absorption at Equilibrium 0.170 - 3.40 %
0.170 - 3.40 %
Average value: 2.26 % Grade Count:83
Water Absorption at Saturation 6.70 - 10.0 %
6.70 - 10.0 %
Average value: 8.33 % Grade Count:25
Maximum Moisture Content 0.100
0.100
Average value: 0.100 Grade Count:6
Linear Mold Shrinkage 0.000100 - 0.0350 cm/cm
0.000100 - 0.0350 in/in
Average value: 0.0127 cm/cm Grade Count:220
Linear Mold Shrinkage, Transverse 0.00200 - 0.0253 cm/cm
0.00200 - 0.0253 in/in
Average value: 0.0156 cm/cm Grade Count:62
Melt Flow 3.00 - 121 g/10 min
3.00 - 121 g/10 min
Average value: 33.7 g/10 min Grade Count:25
Spiral Flow 60.0 - 85.0 cm
23.6 - 33.5 in
Average value: 68.3 cm Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75.0 - 85.0
75.0 - 85.0
Average value: 77.0 Grade Count:5
Hardness, Rockwell R 40.0 - 125
40.0 - 125
Average value: 105 Grade Count:98
Hardness, Shore D 52.0 - 82.0
52.0 - 82.0
Average value: 71.6 Grade Count:16
Ball Indentation Hardness 70.0 - 150 MPa
10200 - 21800 psi
Average value: 109 MPa Grade Count:11
Tensile Strength, Ultimate 22.0 - 200 MPa
3190 - 29000 psi
Average value: 62.0 MPa Grade Count:104
70.0 - 100 MPa

@Temperature -40.0 - -40.0 °C
10200 - 14500 psi

@Temperature -40.0 - -40.0 °F
Average value: 85.0 MPa Grade Count:4
Tensile Strength, Yield 25.0 - 207 MPa
3630 - 30000 psi
Average value: 64.1 MPa Grade Count:188
12.0 - 117 MPa

@Temperature -40.0 - 120 °C
1740 - 17000 psi

@Temperature -40.0 - 248 °F
Average value: 56.9 MPa Grade Count:8
Elongation at Break 1.50 - 500 %
1.50 - 500 %
Average value: 81.1 % Grade Count:241
9.00 - 20.0 %

@Temperature -40.0 - 150 °C
9.00 - 20.0 %

@Temperature -40.0 - 302 °F
Average value: 43.0 % Grade Count:5
Elongation at Yield 3.00 - 350 %
3.00 - 350 %
Average value: 21.7 % Grade Count:88
4.00 - 37.0 %

@Temperature -40.0 - 120 °C
4.00 - 37.0 %

@Temperature -40.0 - 248 °F
Average value: 23.7 % Grade Count:6
Modulus of Elasticity 0.210 - 15.0 GPa
30.5 - 2180 ksi
Average value: 2.32 GPa Grade Count:128
0.145 - 3.30 GPa

@Temperature -40.0 - 150 °C
21.0 - 479 ksi

@Temperature -40.0 - 302 °F
Average value: 0.997 GPa Grade Count:8
Flexural Yield Strength 7.00 - 310 MPa
1020 - 45000 psi
Average value: 84.2 MPa Grade Count:206
8.00 - 148 MPa

@Temperature -40.0 - 120 °C
1160 - 21500 psi

@Temperature -40.0 - 248 °F
Average value: 55.1 MPa Grade Count:8
Flexural Modulus 0.0689 - 12.8 GPa
10.0 - 1860 ksi
Average value: 2.39 GPa Grade Count:236
0.145 - 0.415 GPa

@Temperature 65.0 - 120 °C
21.0 - 60.2 ksi

@Temperature 149 - 248 °F
Average value: 0.262 GPa Grade Count:5
Compressive Yield Strength 24.0 - 120 MPa
3480 - 17400 psi
Average value: 61.6 MPa Grade Count:7
Poissons Ratio 0.350
0.350
Average value: 0.350 Grade Count:6
Izod Impact, Notched 0.0850 J/cm - NB
0.159 ft-lb/in - NB
Average value: 4.49 J/cm Grade Count:155
0.350 - 2.99 J/cm

@Temperature -40.0 - -40.0 °C
0.656 - 5.60 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.52 J/cm Grade Count:12
0.588399 - 5338.47 J/cm

@Temperature -40.0 - -20.0 °C
1.10231 - 10001.1 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 1.52 J/cm Grade Count:22
0.588399 - 5338.47 J/cm

@Thickness 3.17 - 6.40 mm
1.10231 - 10001.1 ft-lb/in

@Thickness 0.125 - 0.252 in
Average value: 1.52 J/cm Grade Count:22
Izod Impact, Unnotched 13.9 J/cm - NB
26.0 ft-lb/in - NB
Average value: 14.6 J/cm Grade Count:35
Izod Impact, Notched (ISO) 8.00 kJ/m² - NB
3.81 ft-lb/in² - NB
Average value: 43.5 kJ/m² Grade Count:57
5.00 - 85.0 kJ/m²

@Temperature -40.0 - -20.0 °C
2.38 - 40.4 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 21.1 kJ/m² Grade Count:31
Izod Impact, Unnotched (ISO) 75.0 kJ/m² - NB
35.7 ft-lb/in² - NB
Average value: 94.5 kJ/m² Grade Count:25
65.0 kJ/m² - NB

@Temperature -30.0 - -30.0 °C
30.9 ft-lb/in² - NB

@Temperature -22.0 - -22.0 °F
Average value: 76.7 kJ/m² Grade Count:15
Charpy Impact Unnotched 2.50 J/cm² - NB
11.9 ft-lb/in² - NB
Average value: 8.56 J/cm² Grade Count:97
4.50 J/cm² - NB

@Temperature -70.0 - -20.0 °C
21.4 ft-lb/in² - NB

@Temperature -94.0 - -4.00 °F
Average value: 8.35 J/cm² Grade Count:51
Charpy Impact, Notched 0.400 J/cm² - NB
1.90 ft-lb/in² - NB
Average value: 4.43 J/cm² Grade Count:103
0.300 - 8.50 J/cm²

@Temperature -40.0 - -20.0 °C
1.43 - 40.5 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 1.86 J/cm² Grade Count:56
Gardner Impact 36.2 J
26.7 ft-lb
Average value: 36.2 J Grade Count:4
Dart Drop, Total Energy 45.0 - 45.0 J

@Temperature -20.0 - -20.0 °C
33.2 - 33.2 ft-lb

@Temperature -4.00 - -4.00 °F
Average value: 45.0 J Grade Count:1
Puncture Energy 50.0 - 65.0 J
36.9 - 47.9 ft-lb
Average value: 60.8 J Grade Count:4
64.0 - 64.0 J

@Temperature -30.0 - -30.0 °C
47.2 - 47.2 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 60.9 J Grade Count:1
50.0 - 67.0 J

@Temperature -30.0 - -30.0 °C
36.9 - 49.4 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 60.9 J Grade Count:3
50.0 - 67.0 J

@Load <=5810 kg
36.9 - 49.4 ft-lb

@Load <=12800 lb
Average value: 60.9 J Grade Count:3
Taber Abrasion, mg/1000 Cycles 8.00 - 19.0
8.00 - 19.0
Average value: 13.5 Grade Count:4
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1.00e+17 ohm-cm
100 - 1.00e+17 ohm-cm
Average value: 1.55e+15 ohm-cm Grade Count:122
Surface Resistance 100 - 1.00e+16 ohm
100 - 1.00e+16 ohm
Average value: 2.50e+14 ohm Grade Count:58
Dielectric Constant 2.70 - 15.4
2.70 - 15.4
Average value: 5.32 Grade Count:53
Dielectric Strength 11.8 - 100 kV/mm
300 - 2540 kV/in
Average value: 26.8 kV/mm Grade Count:105
Dissipation Factor 0.00300 - 0.400
0.00300 - 0.400
Average value: 0.123 Grade Count:22
Dielectric Loss Index 0.0190 - 0.300
0.0190 - 0.300
Average value: 0.132 Grade Count:13