Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.23 - 1.73 g/cc
0.0444 - 0.0625 lb/in³
Average value: 1.45 g/cc Grade Count:117
1.25 - 1.28 g/cc

@Temperature 250 - 270 °C
0.0452 - 0.0462 lb/in³

@Temperature 482 - 518 °F
Average value: 1.26 g/cc Grade Count:2
Filler Content 10.0 - 45.0 %
10.0 - 45.0 %
Average value: 27.9 % Grade Count:26
Water Absorption 0.350 - 5.40 %
0.350 - 5.40 %
Average value: 1.22 % Grade Count:51
Moisture Absorption at Equilibrium 1.10 - 2.00 %
1.10 - 2.00 %
Average value: 1.49 % Grade Count:10
Viscosity 30.0 - 120 cP

@Temperature 280 - 300 °C
30.0 - 120 cP

@Temperature 536 - 572 °F
Average value: 70.7 cP Grade Count:1
30.0 - 120 cP

@Shear Rate 100 - 1000 1/s
30.0 - 120 cP

@Shear Rate 100 - 1000 1/s
Average value: 70.7 cP Grade Count:1
Linear Mold Shrinkage 0.00150 - 0.0500 cm/cm
0.00150 - 0.0500 in/in
Average value: 0.00641 cm/cm Grade Count:111
Linear Mold Shrinkage, Transverse 0.00500 - 0.0140 cm/cm
0.00500 - 0.0140 in/in
Average value: 0.00930 cm/cm Grade Count:32
Melt Flow 2.00 - 44.4 g/10 min
2.00 - 44.4 g/10 min
Average value: 19.4 g/10 min Grade Count:5
Mechanical Properties Metric English Comments
Hardness, Rockwell M 74.0 - 98.0
74.0 - 98.0
Average value: 93.4 Grade Count:7
Hardness, Rockwell R 112 - 122
112 - 122
Average value: 120 Grade Count:35
Tensile Strength, Ultimate 50.0 - 165 MPa
7250 - 23900 psi
Average value: 111 MPa Grade Count:83
25.0 - 70.0 MPa

@Temperature 60.0 - 150 °C
3630 - 10200 psi

@Temperature 140 - 302 °F
Average value: 50.9 MPa Grade Count:2
22.0 - 80.0 MPa

@Temperature 80.0 - 120 °C
3190 - 11600 psi

@Temperature 176 - 248 °F
Average value: 50.9 MPa Grade Count:1
22.0 - 80.0 MPa

@Strain 1.00 - 8.00 %
3190 - 11600 psi

@Strain 1.00 - 8.00 %
Average value: 50.9 MPa Grade Count:1
Tensile Strength, Yield 71.7 - 175 MPa
10400 - 25400 psi
Average value: 121 MPa Grade Count:42
Elongation at Break 1.00 - 12.0 %
1.00 - 12.0 %
Average value: 3.45 % Grade Count:112
2.70 - 20.0 %

@Temperature 60.0 - 150 °C
2.70 - 20.0 %

@Temperature 140 - 302 °F
Average value: 8.90 % Grade Count:2
Elongation at Yield 2.30 - 6.00 %
2.30 - 6.00 %
Average value: 4.36 % Grade Count:4
5.00 - 10.0 %

@Temperature 90.0 - 150 °C
5.00 - 10.0 %

@Temperature 194 - 302 °F
Average value: 7.33 % Grade Count:1
Modulus of Elasticity 3.70 - 13.1 GPa
537 - 1900 ksi
Average value: 8.03 GPa Grade Count:45
0.485 - 8.00 GPa

@Temperature -140 - 250 °C
70.3 - 1160 ksi

@Temperature -220 - 482 °F
Average value: 4.72 GPa Grade Count:4
Flexural Yield Strength 90.0 - 260 MPa
13100 - 37700 psi
Average value: 176 MPa Grade Count:91
Flexural Modulus 3.10 - 12.5 GPa
450 - 1810 ksi
Average value: 7.42 GPa Grade Count:113
Compressive Yield Strength 138 - 255 MPa
20000 - 37000 psi
Average value: 179 MPa Grade Count:6
Poissons Ratio 0.260 - 0.470

@Temperature -40.0 - 121 °C
0.260 - 0.470

@Temperature -40.0 - 250 °F
Average value: 0.383 Grade Count:1
Shear Modulus 1.96 - 2.68 GPa
285 - 388 ksi
Average value: 2.37 GPa Grade Count:3
>= 0.173 GPa

@Temperature -100 - 250 °C
>= 25.1 ksi

@Temperature -148 - 482 °F
Average value: 1.40 GPa Grade Count:2
Izod Impact, Notched 0.267 - 1.33 J/cm
0.500 - 2.50 ft-lb/in
Average value: 0.536 J/cm Grade Count:76
Izod Impact, Unnotched 0.427 - 9.08 J/cm
0.800 - 17.0 ft-lb/in
Average value: 5.03 J/cm Grade Count:32
Izod Impact, Notched (ISO) 2.60 - 16.0 kJ/m²
1.24 - 7.61 ft-lb/in²
Average value: 5.20 kJ/m² Grade Count:31
2.00 - 7.50 kJ/m²

@Temperature -40.0 - -20.0 °C
0.952 - 3.57 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.76 kJ/m² Grade Count:8
Izod Impact, Unnotched (ISO) 40.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
19.0 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 45.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.00 - 9.00 J/cm²
9.52 - 42.8 ft-lb/in²
Average value: 4.88 J/cm² Grade Count:24
2.00 - 5.00 J/cm²

@Temperature -30.0 - -20.0 °C
9.52 - 23.8 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.00 J/cm² Grade Count:11
Charpy Impact, Notched 0.200 - 1.60 J/cm²
0.952 - 7.61 ft-lb/in²
Average value: 0.569 J/cm² Grade Count:28
0.200 - 0.700 J/cm²

@Temperature -40.0 - -20.0 °C
0.952 - 3.33 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.391 J/cm² Grade Count:15
Thermal Properties Metric English Comments
CTE, linear 10.0 - 500 µm/m-°C
5.56 - 278 µin/in-°F
Average value: 55.8 µm/m-°C Grade Count:37
CTE, linear, Transverse to Flow 50.0 - 100 µm/m-°C
27.8 - 55.6 µin/in-°F
Average value: 75.3 µm/m-°C Grade Count:8
Specific Heat Capacity 1.50 - 2.10 J/g-°C
0.359 - 0.502 BTU/lb-°F
Average value: 1.70 J/g-°C Grade Count:5
Thermal Conductivity 0.250 - 0.504 W/m-K
1.74 - 3.50 BTU-in/hr-ft²-°F
Average value: 0.374 W/m-K Grade Count:7
Melting Point 220 - 275 °C
428 - 527 °F
Average value: 259 °C Grade Count:64
Maximum Service Temperature, Air 115 - 254 °C
239 - 489 °F
Average value: 179 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 210 - 263 °C
410 - 505 °F
Average value: 249 °C Grade Count:65
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 - 1.00e+17 ohm-cm
1.00e+9 - 1.00e+17 ohm-cm
Average value: 2.75e+15 ohm-cm Grade Count:44
Surface Resistance 1.00e+10 - 1.00e+14 ohm
1.00e+10 - 1.00e+14 ohm
Average value: 2.21e+13 ohm Grade Count:12
Dielectric Constant 3.00 - 13.9
3.00 - 13.9
Average value: 4.82 Grade Count:14
Dielectric Strength 15.7 - 40.0 kV/mm
400 - 1020 kV/in
Average value: 24.5 kV/mm Grade Count:33
Dissipation Factor 0.0100 - 0.540
0.0100 - 0.540
Average value: 0.0642 Grade Count:8
Dielectric Loss Index 0.0150 - 0.150
0.0150 - 0.150
Average value: 0.0825 Grade Count:4
Arc Resistance 125 - 130 sec
125 - 130 sec
Average value: 128 sec Grade Count:4
Comparative Tracking Index 375 - 600 V
375 - 600 V
Average value: 436 V Grade Count:14