Overview of materials for PEN-PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , PEN-PET
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for PEN-PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.33 - 1.45 g/cc
0.0480 - 0.0524 lb/in³
Average value: 1.35 g/cc Grade Count:6
Water Absorption 0.0600 - 0.150 %
0.0600 - 0.150 %
Average value: 0.0800 % Grade Count:6
Linear Mold Shrinkage 0.00400 - 0.0150 cm/cm
0.00400 - 0.0150 in/in
Average value: 0.00667 cm/cm Grade Count:6
Melt Flow 12.0 - 25.0 g/10 min
12.0 - 25.0 g/10 min
Average value: 16.4 g/10 min Grade Count:5
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88.0 - 115
88.0 - 115
Average value: 96.7 Grade Count:6
Tensile Strength, Ultimate 58.8 - 81.4 MPa
8530 - 11800 psi
Average value: 68.7 MPa Grade Count:6
Elongation at Break 40.0 - 460 %
40.0 - 460 %
Average value: 187 % Grade Count:6
Flexural Yield Strength 63.7 - 92.2 MPa
9250 - 13400 psi
Average value: 85.4 MPa Grade Count:6
Flexural Modulus 2.16 - 3.14 GPa
313 - 455 ksi
Average value: 2.63 GPa Grade Count:6
Izod Impact, Notched 0.412 - 0.539 J/cm
0.772 - 1.01 ft-lb/in
Average value: 0.461 J/cm Grade Count:6
Thermal Properties Metric English Comments
CTE, linear 60.0 - 400 µm/m-°C
33.3 - 222 µin/in-°F
Average value: 117 µm/m-°C Grade Count:6
Melting Point 215 - 255 °C
419 - 491 °F
Average value: 240 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 75.0 - 120 °C
167 - 248 °F
Average value: 96.5 °C Grade Count:6
Glass Transition Temp, Tg 82.0 - 121 °C
180 - 250 °F
Average value: 98.8 °C Grade Count:5
Flammability, UL94 HB - V-2
HB - V-2
Grade Count:6
Optical Properties Metric English Comments
Haze 1.00 - 1.60 %
1.00 - 1.60 %
Average value: 1.22 % Grade Count:5