Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Phenolic, Carbon Fiber Composite

Category Polymer , Thermoset , Phenolic , Phenolic, Carbon Fiber Composite
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Phenolic, Carbon Fiber Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.31 - 1.55 g/cc
0.0473 - 0.0560 lb/in³
Average value: 1.42 g/cc Grade Count:8
Water Absorption 0.0500 - 0.900 %
0.0500 - 0.900 %
Average value: 0.289 % Grade Count:4
Linear Mold Shrinkage 0.000 - 0.00200 cm/cm
0.000 - 0.00200 in/in
Average value: 0.000760 cm/cm Grade Count:5
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 - 258 MPa
7250 - 37400 psi
Average value: 119 MPa Grade Count:8
Modulus of Elasticity 20.0 - 62.0 GPa
2900 - 8990 ksi
Average value: 38.2 GPa Grade Count:3
Flexural Yield Strength 102 - 521 MPa
14800 - 75600 psi
Average value: 253 MPa Grade Count:8
Flexural Modulus 6.30 - 44.8 GPa
914 - 6500 ksi
Average value: 21.8 GPa Grade Count:8
Compressive Yield Strength 164 - 359 MPa
23800 - 52100 psi
Average value: 258 MPa Grade Count:7
Compressive Modulus 8.41 - 17.0 GPa
1220 - 2470 ksi
Average value: 11.9 GPa Grade Count:3
Charpy Impact Unnotched 1.09 - 1.70 J/cm²
5.19 - 8.09 ft-lb/in²
Average value: 1.38 J/cm² Grade Count:3
Charpy Impact, Notched 0.200 - 0.300 J/cm²
0.952 - 1.43 ft-lb/in²
Average value: 0.248 J/cm² Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 1.00 - 10.0 µm/m-°C
0.556 - 5.56 µin/in-°F
Average value: 5.67 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 20.0 - 40.0 µm/m-°C
11.1 - 22.2 µin/in-°F
Average value: 26.5 µm/m-°C Grade Count:3
Copyright © lookpolymers.com All Rights Reserved