Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.47 - 1.61 g/cc
0.0531 - 0.0582 lb/in³
Average value: 1.52 g/cc Grade Count:12
Apparent Bulk Density 0.600 - 0.740 g/cc
0.0217 - 0.0267 lb/in³
Average value: 0.670 g/cc Grade Count:12
Water Absorption 0.200 - 0.300 %
0.200 - 0.300 %
Average value: 0.240 % Grade Count:12
Linear Mold Shrinkage 0.00330 - 0.0120 cm/cm
0.00330 - 0.0120 in/in
Average value: 0.00687 cm/cm Grade Count:12
Mechanical Properties Metric English Comments
Hardness, Rockwell E 79.0 - 87.0
79.0 - 87.0
Average value: 82.0 Grade Count:4
Tensile Strength, Ultimate 41.0 - 60.5 MPa
5950 - 8770 psi
Average value: 50.5 MPa Grade Count:12
Elongation at Break 0.740 - 0.860 %
0.740 - 0.860 %
Average value: 0.813 % Grade Count:4
Modulus of Elasticity 8.80 - 13.1 GPa
1280 - 1900 ksi
Average value: 10.3 GPa Grade Count:6
Flexural Yield Strength 69.0 - 89.8 MPa
10000 - 13000 psi
Average value: 78.9 MPa Grade Count:12
Flexural Modulus 8.16 - 10.4 GPa
1180 - 1510 ksi
Average value: 9.12 GPa Grade Count:10
Compressive Yield Strength 145 - 221 MPa
21000 - 32100 psi
Average value: 195 MPa Grade Count:12
Charpy Impact, Notched 0.170 - 0.210 J/cm²
0.809 - 0.999 ft-lb/in²
Average value: 0.188 J/cm² Grade Count:4
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 - 205 °C
302 - 401 °F
Average value: 186 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 166 - 204 °C
331 - 399 °F
Average value: 180 °C Grade Count:12
UL RTI, Electrical 150 °C
302 °F
Average value: 150 °C Grade Count:6
UL RTI, Mechanical with Impact 150 °C
302 °F
Average value: 150 °C Grade Count:6
UL RTI, Mechanical without Impact 150 °C
302 °F
Average value: 150 °C Grade Count:6
Flammability, UL94 V-1 - 5VA
V-1 - 5VA
Grade Count:12
Electrical Properties Metric English Comments
Electrical Resistivity 1.35e+11 - 2.68e+12 ohm-cm
1.35e+11 - 2.68e+12 ohm-cm
Average value: 9.78e+11 ohm-cm Grade Count:12
Dielectric Constant 4.80 - 14.0
4.80 - 14.0
Average value: 6.62 Grade Count:12
Dielectric Strength 7.40 - 16.7 kV/mm
188 - 424 kV/in
Average value: 12.6 kV/mm Grade Count:12
Dissipation Factor 0.0370 - 0.170
0.0370 - 0.170
Average value: 0.0726 Grade Count:12
Arc Resistance 150 - 180 sec
150 - 180 sec
Average value: 165 sec Grade Count:6
Comparative Tracking Index 175 - 230 V
175 - 230 V
Average value: 193 V Grade Count:12