Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.25 - 2.00 g/cc
0.0452 - 0.0723 lb/in³
Average value: 1.74 g/cc Grade Count:7
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.0 - 290 MPa
10900 - 42000 psi
Average value: 188 MPa Grade Count:7
Flexural Yield Strength 120 - 400 MPa
17400 - 58000 psi
Average value: 257 MPa Grade Count:7
Flexural Modulus 9.00 - 22.0 GPa
1310 - 3190 ksi
Average value: 14.0 GPa Grade Count:6
Compressive Yield Strength 379 - 660 MPa
55000 - 95700 psi
Average value: 488 MPa Grade Count:3
Izod Impact, Notched 2.67 - 6.41 J/cm
5.00 - 12.0 ft-lb/in
Average value: 5.19 J/cm Grade Count:4
Thermal Properties Metric English Comments
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:4
Electrical Properties Metric English Comments
Insulation Resistance 1.00e+8 - 1.00e+9 ohm
1.00e+8 - 1.00e+9 ohm
Average value: 4.00e+8 ohm Grade Count:3
Dielectric Constant 5.00 - 7.30
5.00 - 7.30
Average value: 5.66 Grade Count:4
Dielectric Breakdown >= 20000 V

@Temperature 90.0 - 90.0 °C
>= 20000 V

@Temperature 194 - 194 °F
Average value: 30000 V Grade Count:2
Dissipation Factor 0.0230 - 0.0300
0.0230 - 0.0300
Average value: 0.0282 Grade Count:3
Comparative Tracking Index 100 - 150 V
100 - 150 V
Average value: 117 V Grade Count:3