Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.13 - 1.75 g/cc
0.0408 - 0.0632 lb/in³
Average value: 1.48 g/cc Grade Count:151
Filler Content 15.0 - 35.0 %
15.0 - 35.0 %
Average value: 25.5 % Grade Count:10
Water Absorption 0.000 - 0.600 %
0.000 - 0.600 %
Average value: 0.123 % Grade Count:52
Moisture Absorption at Equilibrium 0.0300 - 0.500 %
0.0300 - 0.500 %
Average value: 0.107 % Grade Count:57
Water Absorption at Saturation 0.350 - 0.500 %
0.350 - 0.500 %
Average value: 0.438 % Grade Count:4
Linear Mold Shrinkage 0.00170 - 0.0260 cm/cm
0.00170 - 0.0260 in/in
Average value: 0.0109 cm/cm Grade Count:137
Linear Mold Shrinkage, Transverse 0.00170 - 0.0300 cm/cm
0.00170 - 0.0300 in/in
Average value: 0.0116 cm/cm Grade Count:27
Melt Flow 3.00 - 82.0 g/10 min
3.00 - 82.0 g/10 min
Average value: 27.0 g/10 min Grade Count:35
Mechanical Properties Metric English Comments
Hardness, Rockwell M 79.0 - 88.0
79.0 - 88.0
Average value: 84.6 Grade Count:5
Hardness, Rockwell R 116 - 124
116 - 124
Average value: 119 Grade Count:30
Tensile Strength, Ultimate 29.0 - 147 MPa
4210 - 21300 psi
Average value: 70.3 MPa Grade Count:77
12.0 - 85.0 MPa

@Temperature 60.0 - 150 °C
1740 - 12300 psi

@Temperature 140 - 302 °F
Average value: 41.5 MPa Grade Count:3
Tensile Strength, Yield 30.0 - 130 MPa
4350 - 18900 psi
Average value: 77.9 MPa Grade Count:91
Elongation at Break 1.00 - 145 %
1.00 - 145 %
Average value: 17.3 % Grade Count:85
4.00 - 90.0 %

@Temperature 60.0 - 150 °C
4.00 - 90.0 %

@Temperature 140 - 302 °F
Average value: 56.9 % Grade Count:3
Elongation at Yield 2.00 - 75.0 %
2.00 - 75.0 %
Average value: 13.0 % Grade Count:27
4.50 - 10.0 %

@Temperature 60.0 - 90.0 °C
4.50 - 10.0 %

@Temperature 140 - 194 °F
Average value: 7.00 % Grade Count:2
Modulus of Elasticity 0.750 - 11.0 GPa
109 - 1600 ksi
Average value: 3.95 GPa Grade Count:46
0.350 - 7.20 GPa

@Temperature 60.0 - 150 °C
50.8 - 1040 ksi

@Temperature 140 - 302 °F
Average value: 2.13 GPa Grade Count:3
Flexural Yield Strength 55.0 - 216 MPa
7980 - 31300 psi
Average value: 127 MPa Grade Count:121
35.0 - 35.0 MPa

@Temperature 90.0 - 90.0 °C
5080 - 5080 psi

@Temperature 194 - 194 °F
Average value: 35.0 MPa Grade Count:1
Flexural Modulus 1.57 - 11.0 GPa
228 - 1600 ksi
Average value: 5.37 GPa Grade Count:127
0.600 - 0.600 GPa

@Temperature 90.0 - 90.0 °C
87.0 - 87.0 ksi

@Temperature 194 - 194 °F
Average value: 0.600 GPa Grade Count:1
Izod Impact, Notched 0.250 - 6.41 J/cm
0.468 - 12.0 ft-lb/in
Average value: 1.05 J/cm Grade Count:69
1.53 - 3.2034 J/cm

@Temperature -40.0 - -30.0 °C
2.87 - 6.0013 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 2.37 J/cm Grade Count:2
Izod Impact, Unnotched 0.588 J/cm - NB
1.10 ft-lb/in - NB
Average value: 7.79 J/cm Grade Count:8
Izod Impact, Notched (ISO) 4.00 - 45.0 kJ/m²
1.90 - 21.4 ft-lb/in²
Average value: 8.51 kJ/m² Grade Count:51
2.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.50 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) 30.0 - 80.0 kJ/m²
14.3 - 38.1 ft-lb/in²
Average value: 52.4 kJ/m² Grade Count:45
42.0 - 42.0 kJ/m²

@Temperature -30.0 - -30.0 °C
20.0 - 20.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 42.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.00 J/cm² - NB
9.52 ft-lb/in² - NB
Average value: 6.08 J/cm² Grade Count:32
2.50 - 999.9 J/cm²

@Temperature -30.0 - -20.0 °C
11.9 - 4759 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 8.16 J/cm² Grade Count:22
Charpy Impact, Notched 0.160 - 4.50 J/cm²
0.761 - 21.4 ft-lb/in²
Average value: 0.723 J/cm² Grade Count:35
0.200 - 1.00 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.620 J/cm² Grade Count:20
Gardner Impact 9.49 - 43.0 J
7.00 - 31.7 ft-lb
Average value: 30.4 J Grade Count:8
Tensile Impact Strength 45.0 - 100 kJ/m²
21.4 - 47.6 ft-lb/in²
Average value: 65.0 kJ/m² Grade Count:3
Tensile Creep Modulus, 1 hour 950 - 3000 MPa
138000 - 435000 psi
Average value: 2310 MPa Grade Count:8
Tensile Creep Modulus, 1000 hours 650 - 1800 MPa
94300 - 261000 psi
Average value: 1460 MPa Grade Count:8
Thermal Properties Metric English Comments
CTE, linear 19.8 - 139 µm/m-°C
11.0 - 77.2 µin/in-°F
Average value: 72.2 µm/m-°C Grade Count:46
124 - 124 µm/m-°C

@Temperature 60.0 - 138 °C
68.9 - 68.9 µin/in-°F

@Temperature 140 - 280 °F
Average value: 124 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 84.0 - 120 µm/m-°C
46.7 - 66.7 µin/in-°F
Average value: 103 µm/m-°C Grade Count:14
Thermal Conductivity 0.173 - 14.0 W/m-K
1.20 - 97.2 BTU-in/hr-ft²-°F
Average value: 3.31 W/m-K Grade Count:4
Melting Point 200 - 240 °C
392 - 464 °F
Average value: 222 °C Grade Count:30
Electrical Properties Metric English Comments
Electrical Resistivity 1e+05 - 1.00e+17 ohm-cm
1e+05 - 1.00e+17 ohm-cm
Average value: 1.51e+16 ohm-cm Grade Count:106
Surface Resistance 1.00e+8 - 1.00e+17 ohm
1.00e+8 - 1.00e+17 ohm
Average value: 3.60e+15 ohm Grade Count:34
Dielectric Constant 2.80 - 4.00
2.80 - 4.00
Average value: 3.25 Grade Count:84
Dielectric Strength 15.0 - 42.9 kV/mm
381 - 1090 kV/in
Average value: 22.3 kV/mm Grade Count:104
Dissipation Factor 0.00100 - 0.0300
0.00100 - 0.0300
Average value: 0.0132 Grade Count:28
Dielectric Loss Index 0.00100 - 0.0200
0.00100 - 0.0200
Average value: 0.0183 Grade Count:44
Arc Resistance 21.0 - 120 sec
21.0 - 120 sec
Average value: 97.1 sec Grade Count:16
Comparative Tracking Index 0.000 - 600 V
0.000 - 600 V
Average value: 339 V Grade Count:34
Hot Wire Ignition, HWI 7.00 - 120 sec
7.00 - 120 sec
Average value: 34.5 sec Grade Count:6
High Amp Arc Ignition, HAI 15.0 - 120 arcs
15.0 - 120 arcs
Average value: 98.0 arcs Grade Count:6
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
Average value: 127 mm/min Grade Count:6