Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Mineral Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.29 - 1.81 g/cc
0.0466 - 0.0654 lb/in³
Average value: 1.50 g/cc Grade Count:34
Water Absorption 0.000 - 0.500 %
0.000 - 0.500 %
Average value: 0.243 % Grade Count:16
Moisture Absorption at Equilibrium 0.150 - 0.500 %
0.150 - 0.500 %
Average value: 0.256 % Grade Count:8
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cm
0.00100 - 0.0200 in/in
Average value: 0.0117 cm/cm Grade Count:27
Linear Mold Shrinkage, Transverse 0.00100 - 0.0190 cm/cm
0.00100 - 0.0190 in/in
Average value: 0.0127 cm/cm Grade Count:11
Melt Flow 9.59 - 58.0 g/10 min
9.59 - 58.0 g/10 min
Average value: 25.7 g/10 min Grade Count:18
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109 - 122
109 - 122
Average value: 115 Grade Count:8
Tensile Strength, Ultimate 45.0 - 105 MPa
6530 - 15200 psi
Average value: 57.6 MPa Grade Count:21
35.0 - 55.0 MPa

@Temperature 60.0 - 120 °C
5080 - 7980 psi

@Temperature 140 - 248 °F
Average value: 43.3 MPa Grade Count:1
Tensile Strength, Yield 30.0 - 103 MPa
4350 - 15000 psi
Average value: 56.9 MPa Grade Count:15
Elongation at Break 2.00 - 80.0 %
2.00 - 80.0 %
Average value: 8.81 % Grade Count:31
Elongation at Yield 3.00 - 7.00 %
3.00 - 7.00 %
Average value: 4.33 % Grade Count:3
Modulus of Elasticity 2.20 - 7.20 GPa
319 - 1040 ksi
Average value: 4.32 GPa Grade Count:20
Flexural Yield Strength 55.0 - 186 MPa
7980 - 27000 psi
Average value: 101 MPa Grade Count:26
Flexural Modulus 1.90 - 9.65 GPa
276 - 1400 ksi
Average value: 4.72 GPa Grade Count:26
2.50 - 5.00 GPa

@Temperature 60.0 - 120 °C
363 - 725 ksi

@Temperature 140 - 248 °F
Average value: 3.67 GPa Grade Count:1
Izod Impact, Notched 0.210 - 1.90 J/cm
0.393 - 3.56 ft-lb/in
Average value: 0.606 J/cm Grade Count:16
0.400 - 0.5339 J/cm

@Temperature -40.0 - -20.0 °C
0.749 - 1.000 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.445 J/cm Grade Count:2
Izod Impact, Unnotched 2.83 - 11.7 J/cm
5.30 - 22.0 ft-lb/in
Average value: 5.27 J/cm Grade Count:4
Izod Impact, Notched (ISO) 5.00 - 15.0 kJ/m²
2.38 - 7.14 ft-lb/in²
Average value: 10.0 kJ/m² Grade Count:3
5.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.50 kJ/m² Grade Count:2
Izod Impact, Unnotched (ISO) 25.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 32.5 kJ/m² Grade Count:2
Charpy Impact Unnotched 1.50 - 1000 J/cm²
7.14 - 4760 ft-lb/in²
Average value: 5.06 J/cm² Grade Count:10
2.50 - 12.0 J/cm²

@Temperature -40.0 - -20.0 °C
11.9 - 57.1 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.81 J/cm² Grade Count:4
Charpy Impact, Notched 0.290 - 1.00 J/cm²
1.38 - 4.76 ft-lb/in²
Average value: 0.471 J/cm² Grade Count:15
0.200 - 1.00 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.480 J/cm² Grade Count:5
Tensile Creep Modulus, 1000 hours 1200 - 2000 MPa
174000 - 290000 psi
Average value: 1500 MPa Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 5.00 - 115 µm/m-°C
2.78 - 63.9 µin/in-°F
Average value: 50.8 µm/m-°C Grade Count:13
61.0 - 61.0 µm/m-°C

@Temperature 60.0 - 138 °C
33.9 - 33.9 µin/in-°F

@Temperature 140 - 280 °F
Average value: 61.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 50.0 - 115 µm/m-°C
27.8 - 63.9 µin/in-°F
Average value: 85.6 µm/m-°C Grade Count:8
88.0 - 88.0 µm/m-°C

@Temperature 60.0 - 138 °C
48.9 - 48.9 µin/in-°F

@Temperature 140 - 280 °F
Average value: 88.0 µm/m-°C Grade Count:1
Melting Point 210 - 225 °C
410 - 437 °F
Average value: 223 °C Grade Count:15
Maximum Service Temperature, Air 100 - 345 °C
212 - 653 °F
Average value: 234 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 110 - 215 °C
230 - 419 °F
Average value: 176 °C Grade Count:30
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 206 °C
120 - 402 °F
Average value: 104 °C Grade Count:29
Vicat Softening Point 170 - 205 °C
338 - 401 °F
Average value: 186 °C Grade Count:6
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:31
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 753 °C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+14 - 4.00e+16 ohm-cm
5.00e+14 - 4.00e+16 ohm-cm
Average value: 7.72e+15 ohm-cm Grade Count:14
Surface Resistance 1.00e+13 - 7.30e+17 ohm
1.00e+13 - 7.30e+17 ohm
Average value: 8.24e+16 ohm Grade Count:9
Dielectric Constant 3.00 - 4.10
3.00 - 4.10
Average value: 3.64 Grade Count:11
Dielectric Strength 14.0 - 100 kV/mm
356 - 2540 kV/in
Average value: 35.8 kV/mm Grade Count:10
Dissipation Factor 0.00120 - 0.0320
0.00120 - 0.0320
Average value: 0.0132 Grade Count:7
Comparative Tracking Index 150 - 425 V
150 - 425 V
Average value: 251 V Grade Count:15
Processing Properties Metric English Comments
Processing Temperature 65.0 - 280 °C
149 - 536 °F
Average value: 221 °C Grade Count:3
Melt Temperature 20.0 - 277 °C
68.0 - 531 °F
Average value: 246 °C Grade Count:16
Mold Temperature 40.0 - 110 °C
104 - 230 °F
Average value: 74.3 °C Grade Count:13
Drying Temperature 116 - 140 °C
240 - 284 °F
Average value: 124 °C Grade Count:8
Moisture Content 0.000 - 0.200 %
0.000 - 0.200 %
Average value: 0.0625 % Grade Count:4
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved