Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.19 - 1.20 g/cc
0.0430 - 0.0434 lb/in³
Average value: 1.20 g/cc Grade Count:17
Water Absorption 0.150 - 0.350 %
0.150 - 0.350 %
Average value: 0.183 % Grade Count:7
Moisture Absorption at Equilibrium 0.150 - 0.350 %
0.150 - 0.350 %
Average value: 0.271 % Grade Count:7
0.580 - 0.580 %

@Temperature 100 - 100 °C
0.580 - 0.580 %

@Temperature 212 - 212 °F
Average value: 0.580 % Grade Count:1
Water Absorption at Saturation 0.160 - 0.350 %
0.160 - 0.350 %
Average value: 0.255 % Grade Count:6
Linear Mold Shrinkage 0.00500 - 0.00800 cm/cm
0.00500 - 0.00800 in/in
Average value: 0.00628 cm/cm Grade Count:15
Melt Flow 3.00 - 112 g/10 min
3.00 - 112 g/10 min
Average value: 15.2 g/10 min Grade Count:16
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70.0 - 85.0
70.0 - 85.0
Average value: 73.8 Grade Count:12
Hardness, Rockwell R 118 - 122
118 - 122
Average value: 119 Grade Count:15
Tensile Strength, Ultimate 65.0 - 75.0 MPa
9430 - 10900 psi
Average value: 68.7 MPa Grade Count:16
Tensile Strength, Yield 60.0 - 65.0 MPa
8700 - 9430 psi
Average value: 63.1 MPa Grade Count:17
Elongation at Break 7.00 - 150 %
7.00 - 150 %
Average value: 109 % Grade Count:17
Elongation at Yield 6.00 - 7.00 %
6.00 - 7.00 %
Average value: 6.50 % Grade Count:16
Modulus of Elasticity 2.09 - 2.43 GPa
303 - 352 ksi
Average value: 2.27 GPa Grade Count:8
Flexural Yield Strength 66.0 - 97.9 MPa
9570 - 14200 psi
Average value: 90.5 MPa Grade Count:14
Flexural Modulus 2.02 - 2.34 GPa
293 - 340 ksi
Average value: 2.22 GPa Grade Count:14
Izod Impact, Notched 6.40 - 9.08 J/cm
12.0 - 17.0 ft-lb/in
Average value: 7.61 J/cm Grade Count:16
1.39 - 1.44 J/cm

@Temperature -30.0 - -30.0 °C
2.60 - 2.70 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 1.43 J/cm Grade Count:4
Izod Impact, Unnotched 32.0 J/cm - NB
60.0 ft-lb/in - NB
Average value: 32.0 J/cm Grade Count:8
Izod Impact, Notched (ISO) 13.0 - 70.0 kJ/m²
6.19 - 33.3 ft-lb/in²
Average value: 39.8 kJ/m² Grade Count:5
10.0 - 12.0 kJ/m²

@Temperature -30.0 - -30.0 °C
4.76 - 5.71 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 10.8 kJ/m² Grade Count:5
Izod Impact, Unnotched (ISO) NB - NB

@Temperature -30.0 - -30.0 °C
NB - NB

@Temperature -22.0 - -22.0 °F
Grade Count:2
Charpy Impact Unnotched 1000 J/cm² - NB
4760 ft-lb/in² - NB
Grade Count:5
999.9 - 999.9 J/cm²

@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Grade Count:2
Charpy Impact, Notched 1.20 - 9.50 J/cm²
5.71 - 45.2 ft-lb/in²
Average value: 4.64 J/cm² Grade Count:7
1.00 - 1.50 J/cm²

@Temperature -30.0 - -30.0 °C
4.76 - 7.14 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.33 J/cm² Grade Count:2
Gardner Impact 36.2 J
26.7 ft-lb
Average value: 36.2 J Grade Count:8
Tensile Impact Strength 378 - 589 kJ/m²
180 - 280 ft-lb/in²
Average value: 541 kJ/m² Grade Count:6
Dart Drop, Total Energy 149 - 169 J
110 - 125 ft-lb
Average value: 154 J Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 55.8 - 91.8 µm/m-°C
31.0 - 51.0 µin/in-°F
Average value: 69.2 µm/m-°C Grade Count:9
CTE, linear, Transverse to Flow 57.0 - 70.0 µm/m-°C
31.7 - 38.9 µin/in-°F
Average value: 62.3 µm/m-°C Grade Count:6
Specific Heat Capacity 1.25 J/g-°C
0.299 BTU/lb-°F
Average value: 1.25 J/g-°C Grade Count:4
Thermal Conductivity 0.190 - 0.210 W/m-K
1.32 - 1.46 BTU-in/hr-ft²-°F
Average value: 0.204 W/m-K Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 128 - 160 °C
262 - 320 °F
Average value: 136 °C Grade Count:13
Deflection Temperature at 1.8 MPa (264 psi) 122 - 151 °C
252 - 304 °F
Average value: 131 °C Grade Count:16
Vicat Softening Point 140 - 160 °C
284 - 320 °F
Average value: 150 °C Grade Count:16
UL RTI, Electrical 125 - 130 °C
257 - 266 °F
Average value: 126 °C Grade Count:4
UL RTI, Mechanical with Impact 125 - 130 °C
257 - 266 °F
Average value: 126 °C Grade Count:4
UL RTI, Mechanical without Impact 125 - 130 °C
257 - 266 °F
Average value: 126 °C Grade Count:4
Flammability, UL94 V-2
V-2
Grade Count:10
Optical Properties Metric English Comments
Refractive Index 1.59 - 1.60
1.59 - 1.60
Average value: 1.60 Grade Count:4
Haze 1.00 - 1.10 %
1.00 - 1.10 %
Average value: 1.01 % Grade Count:14
Transmission, Visible 85.0 - 89.0 %
85.0 - 89.0 %
Average value: 86.8 % Grade Count:6
UV Transmittance 88.0 %
88.0 %
Average value: 88.0 % Grade Count:8
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 - 2.60e+17 ohm-cm
1.00e+17 - 2.60e+17 ohm-cm
Average value: 2.13e+17 ohm-cm Grade Count:6
Dielectric Constant 2.70 - 3.17
2.70 - 3.17
Average value: 2.98 Grade Count:6
Dielectric Strength 14.9 - 20.2 kV/mm
378 - 513 kV/in
Average value: 17.9 kV/mm Grade Count:6
Dissipation Factor 0.000500 - 0.0240
0.000500 - 0.0240
Average value: 0.00728 Grade Count:6
Comparative Tracking Index 175 - 250 V
175 - 250 V
Average value: 213 V Grade Count:3
Hot Wire Ignition, HWI 30.0 - 60.0 sec
30.0 - 60.0 sec
Average value: 45.0 sec Grade Count:3
High Amp Arc Ignition, HAI 0.000 - 15.0 arcs
0.000 - 15.0 arcs
Average value: 7.50 arcs Grade Count:3
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
Average value: 115 mm/min Grade Count:3
Processing Properties Metric English Comments
Melt Temperature 249 - 343 °C
480 - 650 °F
Average value: 293 °C Grade Count:8
Mold Temperature 65.6 - 116 °C
150 - 240 °F
Average value: 85.7 °C Grade Count:8
Drying Temperature 118 - 124 °C
245 - 255 °F
Average value: 121 °C Grade Count:8