Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate/PET Polyester Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.16 - 1.40 g/cc
0.0419 - 0.0506 lb/in³
Average value: 1.21 g/cc Grade Count:125
1.03 - 1.03 g/cc

@Temperature 270 - 270 °C
0.0372 - 0.0372 lb/in³

@Temperature 518 - 518 °F
Average value: 1.03 g/cc Grade Count:1
Water Absorption 0.100 - 0.350 %
0.100 - 0.350 %
Average value: 0.174 % Grade Count:18
Moisture Absorption at Equilibrium 0.0100 - 0.700 %
0.0100 - 0.700 %
Average value: 0.174 % Grade Count:50
Water Absorption at Saturation 0.0100 - 0.700 %
0.0100 - 0.700 %
Average value: 0.327 % Grade Count:50
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.00669 cm/cm Grade Count:113
Linear Mold Shrinkage, Transverse 0.00300 - 0.0100 cm/cm
0.00300 - 0.0100 in/in
Average value: 0.00600 cm/cm Grade Count:47
Melt Flow 3.00 - 44.0 g/10 min
3.00 - 44.0 g/10 min
Average value: 15.4 g/10 min Grade Count:106
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108 - 120
108 - 120
Average value: 115 Grade Count:16
Hardness, Shore D 73.0 - 75.0
73.0 - 75.0
Average value: 73.4 Grade Count:9
Tensile Strength, Ultimate 35.0 - 110 MPa
5080 - 16000 psi
Average value: 55.1 MPa Grade Count:85
Tensile Strength, Yield 34.0 - 70.0 MPa
4930 - 10200 psi
Average value: 53.9 MPa Grade Count:117
Elongation at Break 4.00 - 200 %
4.00 - 200 %
Average value: 127 % Grade Count:97
Elongation at Yield 2.00 - 86.0 %
2.00 - 86.0 %
Average value: 6.30 % Grade Count:75
Modulus of Elasticity 1.16 - 4.15 GPa
168 - 602 ksi
Average value: 1.97 GPa Grade Count:72
Flexural Yield Strength 50.0 - 131 MPa
7250 - 19000 psi
Average value: 81.2 MPa Grade Count:108
Flexural Modulus 1.14 - 5.10 GPa
165 - 740 ksi
Average value: 2.06 GPa Grade Count:118
Izod Impact, Notched 0.392 - 100 J/cm
0.735 - 187 ft-lb/in
Average value: 7.09 J/cm Grade Count:113
0.0500 - 7.50 J/cm

@Temperature -40.0 - 0.000 °C
0.0937 - 14.1 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 2.43 J/cm Grade Count:55
1.60 - 7.50 J/cm

@Temperature -40.0 - -22.0 °C
3.00 - 14.1 ft-lb/in

@Temperature -40.0 - -7.60 °F
Average value: 2.43 J/cm Grade Count:5
1.60 - 7.50 J/cm

@Thickness 3.17 - 3.20 mm
3.00 - 14.1 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 2.43 J/cm Grade Count:5
Izod Impact, Unnotched 5.88 J/cm - NB
11.0 ft-lb/in - NB
Average value: 9.91 J/cm Grade Count:8
99.99 J/cm - NB

@Temperature -40.0 - -30.0 °C
187.3 ft-lb/in - NB

@Temperature -40.0 - -22.0 °F
Grade Count:3
Izod Impact, Notched (ISO) 7.00 - 78.0 kJ/m²
3.33 - 37.1 ft-lb/in²
Average value: 19.7 kJ/m² Grade Count:59
3.00 - 60.0 kJ/m²

@Temperature -40.0 - 0.000 °C
1.43 - 28.6 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 10.7 kJ/m² Grade Count:54
Izod Impact, Unnotched (ISO) 100 kJ/m² - NB
47.6 ft-lb/in² - NB
Average value: 105 kJ/m² Grade Count:4
74.0 kJ/m² - NB

@Temperature -30.0 - -30.0 °C
35.2 ft-lb/in² - NB

@Temperature -22.0 - -22.0 °F
Average value: 77.0 kJ/m² Grade Count:4
Charpy Impact Unnotched 9.50 J/cm² - NB
45.2 ft-lb/in² - NB
Average value: 9.50 J/cm² Grade Count:11
9.50 J/cm² - NB

@Temperature -30.0 - -30.0 °C
45.2 ft-lb/in² - NB

@Temperature -22.0 - -22.0 °F
Average value: 9.50 J/cm² Grade Count:10
Charpy Impact, Notched 0.600 - 9.00 J/cm²
2.86 - 42.8 ft-lb/in²
Average value: 3.19 J/cm² Grade Count:60
0.500 - 5.00 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.79 J/cm² Grade Count:9
Gardner Impact 36.2 - 36.2 J
26.7 - 26.7 ft-lb
Average value: 36.2 J Grade Count:10
Dart Drop, Total Energy 5.31 - 95.0 J
3.92 - 70.1 ft-lb
Average value: 74.9 J Grade Count:46
5.13856 - 5.13856 J

@Temperature -40.0 - -40.0 °C
3.79000 - 3.79000 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 55.4 J Grade Count:1
49.0 - 80.2 J

@Temperature -40.0 - 0.000 °C
36.1 - 59.2 ft-lb

@Temperature -40.0 - 32.0 °F
Average value: 55.4 J Grade Count:2
49.0 - 80.2 J

@Thickness 3.20 - 3.20 mm
36.1 - 59.2 ft-lb

@Thickness 0.126 - 0.126 in
Average value: 55.4 J Grade Count:2
Puncture Energy 49.0 - 49.0 J

@Temperature -40.0 - -40.0 °C
36.1 - 36.1 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 49.0 J Grade Count:2
Thermal Properties Metric English Comments
CTE, linear 26.0 - 120 µm/m-°C
14.4 - 66.7 µin/in-°F
Average value: 85.4 µm/m-°C Grade Count:71
CTE, linear, Transverse to Flow 51.0 - 140 µm/m-°C
28.3 - 77.8 µin/in-°F
Average value: 87.9 µm/m-°C Grade Count:63
Specific Heat Capacity 1.34 - 1.76 J/g-°C
0.320 - 0.421 BTU/lb-°F
Average value: 1.54 J/g-°C Grade Count:3
Thermal Conductivity 0.165 - 0.230 W/m-K
1.15 - 1.60 BTU-in/hr-ft²-°F
Average value: 0.226 W/m-K Grade Count:15
Melting Point 220 - 280 °C
428 - 536 °F
Average value: 246 °C Grade Count:5
Hot Ball Pressure Test 85.0 - 105 °C
185 - 221 °F
Average value: 89.4 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 79.0 - 255 °C
174 - 491 °F
Average value: 110 °C Grade Count:82
Deflection Temperature at 1.8 MPa (264 psi) 40.6 - 222 °C
105 - 432 °F
Average value: 95.5 °C Grade Count:109
Electrical Properties Metric English Comments
Electrical Resistivity 12.0 - 1.00e+17 ohm-cm
12.0 - 1.00e+17 ohm-cm
Average value: 2.36e+16 ohm-cm Grade Count:20
Surface Resistance 12.0 - 1.00e+15 ohm
12.0 - 1.00e+15 ohm
Average value: 8.00e+14 ohm Grade Count:15
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:3
Dielectric Constant 3.00 - 3.20
3.00 - 3.20
Average value: 3.07 Grade Count:3
Dielectric Strength 17.3 - 28.0 kV/mm
439 - 711 kV/in
Average value: 24.9 kV/mm Grade Count:7
Dissipation Factor 0.00800 - 0.00900
0.00800 - 0.00900
Average value: 0.00867 Grade Count:3
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 121 sec Grade Count:4
Comparative Tracking Index 250 - 600 V
250 - 600 V
Average value: 575 V Grade Count:11