Overview of materials for Polycarbonate/Styrenic Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Styrenic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate/Styrenic Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.08 - 1.13 g/cc
0.0390 - 0.0408 lb/in³
Average value: 1.11 g/cc Grade Count:5
Linear Mold Shrinkage 0.00400 cm/cm
0.00400 in/in
Average value: 0.00400 cm/cm Grade Count:5
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92.0 - 120
92.0 - 120
Average value: 111 Grade Count:5
Tensile Strength, Ultimate 48.0 - 76.0 MPa
6960 - 11000 psi
Average value: 61.4 MPa Grade Count:5
Elongation at Break 14.0 - 160 %
14.0 - 160 %
Average value: 65.8 % Grade Count:5
Flexural Yield Strength 68.0 - 131 MPa
9860 - 19000 psi
Average value: 100 MPa Grade Count:5
Flexural Modulus 2.00 - 2.90 GPa
290 - 421 ksi
Average value: 2.54 GPa Grade Count:5
Izod Impact, Notched 0.690 - 6.57 J/cm
1.29 - 12.3 ft-lb/in
Average value: 4.11 J/cm Grade Count:5
Izod Impact, Unnotched 8.01 J/cm - NB
15.0 ft-lb/in - NB
Average value: 8.54 J/cm Grade Count:5
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 - 138 °C
255 - 280 °F
Average value: 130 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 102 - 116 °C
216 - 241 °F
Average value: 109 °C Grade Count:5
Glass Transition Temp, Tg 145 - 150 °C
293 - 302 °F
Average value: 148 °C Grade Count:5
Processing Properties Metric English Comments
Melt Temperature 246 - 277 °C
475 - 531 °F
Average value: 262 °C Grade Count:5