Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.32 - 1.75 g/cc
0.0477 - 0.0632 lb/in³
Average value: 1.59 g/cc Grade Count:68
Filler Content 30.0 %
30.0 %
Average value: 30.0 % Grade Count:9
Water Absorption 0.0400 - 0.700 %
0.0400 - 0.700 %
Average value: 0.160 % Grade Count:23
Moisture Absorption at Equilibrium 0.0500 - 0.240 %
0.0500 - 0.240 %
Average value: 0.169 % Grade Count:19
Viscosity 110000 - 4.11e+6 cP

@Temperature 275 - 305 °C
110000 - 4.11e+6 cP

@Temperature 527 - 581 °F
Average value: 999000 cP Grade Count:3
110000 - 4.11e+6 cP

@Shear Rate 7.30 - 3090 1/s
110000 - 4.11e+6 cP

@Shear Rate 7.30 - 3090 1/s
Average value: 999000 cP Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0110 cm/cm
0.00100 - 0.0110 in/in
Average value: 0.00334 cm/cm Grade Count:62
Linear Mold Shrinkage, Transverse 0.00300 - 0.0105 cm/cm
0.00300 - 0.0105 in/in
Average value: 0.00811 cm/cm Grade Count:30
Melt Flow 5.00 - 65.0 g/10 min
5.00 - 65.0 g/10 min
Average value: 16.8 g/10 min Grade Count:6
Ash 30.0 - 84.0 %
30.0 - 84.0 %
Average value: 49.7 % Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70.0 - 123
70.0 - 123
Average value: 99.4 Grade Count:12
Hardness, Rockwell R 115 - 122
115 - 122
Average value: 119 Grade Count:21
Tensile Strength, Ultimate 67.6 - 170 MPa
9800 - 24700 psi
Average value: 141 MPa Grade Count:54
54.0 - 211 MPa

@Temperature -40.0 - 150 °C
7830 - 30600 psi

@Temperature -40.0 - 302 °F
Average value: 78.5 MPa Grade Count:5
20.5 - 184 MPa

@Temperature -40.0 - 150 °C
2970 - 26700 psi

@Temperature -40.0 - 302 °F
Average value: 78.5 MPa Grade Count:1
20.5 - 184 MPa

@Strain 0.230 - 10.5 %
2970 - 26700 psi

@Strain 0.230 - 10.5 %
Average value: 78.5 MPa Grade Count:1
Tensile Strength, Yield 0.971 - 162 MPa
141 - 23500 psi
Average value: 118 MPa Grade Count:15
Elongation at Break 1.50 - 6.60 %
1.50 - 6.60 %
Average value: 2.64 % Grade Count:59
2.10 - 11.0 %

@Temperature -40.0 - 150 °C
2.10 - 11.0 %

@Temperature -40.0 - 302 °F
Average value: 5.39 % Grade Count:4
Modulus of Elasticity 4.27 - 13.5 GPa
620 - 1960 ksi
Average value: 10.5 GPa Grade Count:33
2.70 - 11.2 GPa

@Temperature -40.0 - 150 °C
392 - 1620 ksi

@Temperature -40.0 - 302 °F
Average value: 6.24 GPa Grade Count:4
Flexural Yield Strength 90.0 - 270 MPa
13100 - 39200 psi
Average value: 206 MPa Grade Count:49
60.0 - 276 MPa

@Temperature -40.0 - 150 °C
8700 - 40000 psi

@Temperature -40.0 - 302 °F
Average value: 150 MPa Grade Count:3
Flexural Modulus 3.65 - 11.4 GPa
530 - 1650 ksi
Average value: 9.18 GPa Grade Count:50
2.25 - 9.66 GPa

@Temperature -40.0 - 150 °C
326 - 1400 ksi

@Temperature -40.0 - 302 °F
Average value: 4.77 GPa Grade Count:3
Compressive Yield Strength 148 - 241 MPa
21500 - 35000 psi
Average value: 193 MPa Grade Count:5
Shear Modulus >= 0.144 GPa

@Temperature -50.0 - 250 °C
>= 20.9 ksi

@Temperature -58.0 - 482 °F
Average value: 1.18 GPa Grade Count:1
Izod Impact, Notched 0.490 - 1.82 J/cm
0.919 - 3.40 ft-lb/in
Average value: 0.880 J/cm Grade Count:45
0.850 - 1.01 J/cm

@Temperature -40.0 - -40.0 °C
1.59 - 1.89 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.930 J/cm Grade Count:2
Izod Impact, Unnotched 0.883 - 9.60 J/cm
1.65 - 18.0 ft-lb/in
Average value: 5.64 J/cm Grade Count:10
6.40 - 9.60 J/cm

@Temperature -40.0 - -40.0 °C
12.0 - 18.0 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 8.00 J/cm Grade Count:2
Izod Impact, Notched (ISO) 7.00 - 18.0 kJ/m²
3.33 - 8.57 ft-lb/in²
Average value: 9.87 kJ/m² Grade Count:22
6.00 - 9.00 kJ/m²

@Temperature -40.0 - -30.0 °C
2.86 - 4.28 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 7.55 kJ/m² Grade Count:11
Izod Impact, Unnotched (ISO) 30.0 - 55.0 kJ/m²
14.3 - 26.2 ft-lb/in²
Average value: 39.4 kJ/m² Grade Count:9
25.0 - 45.0 kJ/m²

@Temperature -40.0 - -30.0 °C
11.9 - 21.4 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 34.4 kJ/m² Grade Count:8
Charpy Impact Unnotched 2.70 - 7.00 J/cm²
12.8 - 33.3 ft-lb/in²
Average value: 4.88 J/cm² Grade Count:13
2.80 - 8.60 J/cm²

@Temperature -40.0 - -30.0 °C
13.3 - 40.9 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.50 J/cm² Grade Count:8
Charpy Impact, Notched 0.850 - 1.60 J/cm²
4.05 - 7.61 ft-lb/in²
Average value: 1.06 J/cm² Grade Count:14
0.800 - 1.20 J/cm²

@Temperature -40.0 - -30.0 °C
3.81 - 5.71 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.945 J/cm² Grade Count:9
Thermal Properties Metric English Comments
CTE, linear 10.0 - 500 µm/m-°C
5.56 - 278 µin/in-°F
Average value: 153 µm/m-°C Grade Count:22
4.00 - 500 µm/m-°C

@Temperature 55.0 - 160 °C
2.22 - 278 µin/in-°F

@Temperature 131 - 320 °F
Average value: 376 µm/m-°C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 - 3.30e+17 ohm-cm
1.00e+13 - 3.30e+17 ohm-cm
Average value: 2.04e+16 ohm-cm Grade Count:34
Surface Resistance 1.00e+13 - 3.00e+15 ohm
1.00e+13 - 3.00e+15 ohm
Average value: 4.48e+14 ohm Grade Count:19
Dielectric Constant 2.83 - 4.80
2.83 - 4.80
Average value: 3.68 Grade Count:27
Dielectric Strength 19.3 - 40.0 kV/mm
490 - 1020 kV/in
Average value: 25.1 kV/mm Grade Count:28
12.0 - 24.0 kV/mm

@Temperature 95.0 - 200 °C
305 - 610 kV/in

@Temperature 203 - 392 °F
Average value: 18.9 kV/mm Grade Count:2
12.0 - 24.0 kV/mm

@Thickness 1.57 - 3.20 mm
305 - 610 kV/in

@Thickness 0.0618 - 0.126 in
Average value: 18.9 kV/mm Grade Count:2
Dissipation Factor 0.00100 - 0.0210
0.00100 - 0.0210
Average value: 0.0125 Grade Count:16
Arc Resistance 77.0 - 129 sec
77.0 - 129 sec
Average value: 109 sec Grade Count:13
Comparative Tracking Index 15.0 - 400 V
15.0 - 400 V
Average value: 225 V Grade Count:20