Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded

Category Polymer , Thermoplastic , Fluoropolymer , PFA , Polyperfluoroalkoxyethylene, Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 2.10 - 2.17 g/cc
0.0759 - 0.0784 lb/in³
Average value: 2.14 g/cc Grade Count:22
Water Absorption 0.0100 - 0.0500 %
0.0100 - 0.0500 %
Average value: 0.0239 % Grade Count:18
Viscosity 1.00e+6 - 1.00e+7 cP

@Temperature 380 - 380 °C
1.00e+6 - 1.00e+7 cP

@Temperature 716 - 716 °F
Average value: 5.50e+6 cP Grade Count:5
Thickness 12.7 - 10000 microns
0.500 - 394 mil
Average value: 1440 microns Grade Count:15
Linear Mold Shrinkage 0.0200 - 0.0600 cm/cm
0.0200 - 0.0600 in/in
Average value: 0.0386 cm/cm Grade Count:7
Melt Flow 1.00 - 36.0 g/10 min
1.00 - 36.0 g/10 min
Average value: 12.2 g/10 min Grade Count:17
Mechanical Properties Metric English Comments
Hardness, Shore D 55.0 - 65.0
55.0 - 65.0
Average value: 60.0 Grade Count:17
Tensile Strength, Ultimate 22.0 - 39.0 MPa
3190 - 5660 psi
Average value: 31.6 MPa Grade Count:18
7.00 - 17.0 MPa

@Temperature 250 - 250 °C
1020 - 2470 psi

@Temperature 482 - 482 °F
Average value: 11.0 MPa Grade Count:8
Elongation at Break 250 - 420 %
250 - 420 %
Average value: 352 % Grade Count:18
400 - 740 %

@Temperature 250 - 250 °C
400 - 740 %

@Temperature 482 - 482 °F
Average value: 622 % Grade Count:9
Modulus of Elasticity 0.276 - 0.700 GPa
40.0 - 102 ksi
Average value: 0.454 GPa Grade Count:8
Flexural Modulus 0.540 - 0.700 GPa
78.3 - 102 ksi
Average value: 0.622 GPa Grade Count:17
Compressive Yield Strength 5.00 - 15.2 MPa
725 - 2200 psi
Average value: 7.11 MPa Grade Count:6
Izod Impact, Notched 100 J/cm - NB
187 ft-lb/in - NB
Grade Count:11
Izod Impact, Unnotched NB
NB
Grade Count:5
NB - NB

@Temperature -40.0 - -40.0 °C
NB - NB

@Temperature -40.0 - -40.0 °F
Grade Count:1
Charpy Impact Unnotched NB - NB

@Temperature -40.0 - -40.0 °C
NB - NB

@Temperature -40.0 - -40.0 °F
Grade Count:1
Coefficient of Friction 0.0400 - 0.250
0.0400 - 0.250
Average value: 0.0932 Grade Count:34
Coefficient of Friction, Static 0.0500
0.0500
Average value: 0.0500 Grade Count:5
Taber Abrasion, mg/1000 Cycles 5.00 - 96.8
5.00 - 96.8
Average value: 61.0 Grade Count:15
Thermal Properties Metric English Comments
CTE, linear 120 - 140 µm/m-°C
66.7 - 77.8 µin/in-°F
Average value: 126 µm/m-°C Grade Count:16
140 - 250 µm/m-°C

@Temperature 100 - 200 °C
77.8 - 139 µin/in-°F

@Temperature 212 - 392 °F
Average value: 195 µm/m-°C Grade Count:1
Specific Heat Capacity 1.05 J/g-°C
0.250 BTU/lb-°F
Average value: 1.05 J/g-°C Grade Count:8
Thermal Conductivity 0.150 - 0.251 W/m-K
1.04 - 1.74 BTU-in/hr-ft²-°F
Average value: 0.238 W/m-K Grade Count:11
Melting Point 300 - 315 °C
572 - 599 °F
Average value: 307 °C Grade Count:16
Maximum Service Temperature, Air 260 °C
500 °F
Average value: 260 °C Grade Count:17
Flammability, UL94 V-0
V-0
Grade Count:34
Oxygen Index 95.0 %
95.0 %
Average value: 95.0 % Grade Count:35
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 - 1.00e+18 ohm-cm
1.00e+17 - 1.00e+18 ohm-cm
Average value: 8.94e+17 ohm-cm Grade Count:17
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
Average value: 1.00e+17 ohm Grade Count:9
Dielectric Constant 1.90 - 2.12
1.90 - 2.12
Average value: 2.06 Grade Count:35
Dielectric Strength 19.7 - 80.0 kV/mm
500 - 2030 kV/in
Average value: 36.3 kV/mm Grade Count:9
Dissipation Factor 0.0000100 - 0.00800
0.0000100 - 0.00800
Average value: 0.000249 Grade Count:34
Arc Resistance 300 sec
300 sec
Average value: 300 sec Grade Count:8
Copyright © lookpolymers.com All Rights Reserved