Overview of materials for Polyphenylene Sulfide (PPS) Coating Resin

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) Coating Resin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphenylene Sulfide (PPS) Coating Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "PPS Coating Resin". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Water Absorption 0.0200 - 0.500 %
0.0200 - 0.500 %
Average value: 0.0900 % Grade Count:7
Melt Flow 45.0 - 600 g/10 min
45.0 - 600 g/10 min
Average value: 247 g/10 min Grade Count:5
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 - 220 °C
320 - 428 °F
Average value: 193 °C Grade Count:6