Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.29 - 3.70 g/cc
0.0466 - 0.134 lb/in³
Average value: 1.70 g/cc Grade Count:18
Filler Content 15.0 - 40.0 %
15.0 - 40.0 %
Average value: 27.9 % Grade Count:7
Water Absorption 0.0200 - 0.200 %
0.0200 - 0.200 %
Average value: 0.0600 % Grade Count:6
Linear Mold Shrinkage 0.000 - 0.00600 cm/cm
0.000 - 0.00600 in/in
Average value: 0.00210 cm/cm Grade Count:18
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116 - 120
116 - 120
Average value: 118 Grade Count:6
Tensile Strength, Ultimate 45.0 - 172 MPa
6530 - 25000 psi
Average value: 112 MPa Grade Count:16
Elongation at Break 0.300 - 100 %
0.300 - 100 %
Average value: 6.78 % Grade Count:18
Modulus of Elasticity 11.0 - 26.2 GPa
1600 - 3800 ksi
Average value: 17.2 GPa Grade Count:9
Flexural Yield Strength 86.2 - 241 MPa
12500 - 35000 psi
Average value: 181 MPa Grade Count:17
Flexural Modulus 0.552 - 25.5 GPa
80.0 - 3700 ksi
Average value: 14.4 GPa Grade Count:18
Izod Impact, Notched 0.267 - 0.854 J/cm
0.500 - 1.60 ft-lb/in
Average value: 0.483 J/cm Grade Count:9
Izod Impact, Unnotched 0.747 - 4.00 J/cm
1.40 - 7.49 ft-lb/in
Average value: 2.26 J/cm Grade Count:10
Thermal Properties Metric English Comments
CTE, linear 19.8 µm/m-°C
11.0 µin/in-°F
Average value: 19.8 µm/m-°C Grade Count:3
Melting Point 280 - 290 °C
536 - 554 °F
Average value: 283 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 260 - 274 °C
500 - 525 °F
Average value: 266 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 220 - 268 °C
428 - 514 °F
Average value: 250 °C Grade Count:10
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:7
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 ohm-cm - 1e+05
1.00 ohm-cm - 1e+05
Average value: 180 ohm-cm Grade Count:16
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 48800 ohm Grade Count:16
Static Decay 0.500 - 2.00 sec
0.500 - 2.00 sec
Average value: 1.81 sec Grade Count:8
Processing Properties Metric English Comments
Melt Temperature 307 - 329 °C
585 - 625 °F
Average value: 319 °C Grade Count:9
Mold Temperature 135 - 177 °C
275 - 350 °F
Average value: 156 °C Grade Count:9
Drying Temperature 149 °C
300 °F
Average value: 149 °C Grade Count:9
Moisture Content 0.0400 %
0.0400 %
Average value: 0.0400 % Grade Count:9
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:9