Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 20% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.20 - 1.64 g/cc
0.0434 - 0.0592 lb/in³
Average value: 1.38 g/cc Grade Count:36
Filler Content 15.0 - 23.0 %
15.0 - 23.0 %
Average value: 18.4 % Grade Count:21
Water Absorption 0.160 - 0.300 %
0.160 - 0.300 %
Average value: 0.233 % Grade Count:17
Linear Mold Shrinkage 0.00200 - 0.0110 cm/cm
0.00200 - 0.0110 in/in
Average value: 0.00518 cm/cm Grade Count:34
Linear Mold Shrinkage, Transverse 0.00600 - 0.0160 cm/cm
0.00600 - 0.0160 in/in
Average value: 0.00843 cm/cm Grade Count:14
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124 - 127
124 - 127
Average value: 125 Grade Count:9
Tensile Strength, Ultimate 9.25 - 200 MPa
1340 - 29000 psi
Average value: 101 MPa Grade Count:35
55.0 - 105 MPa

@Temperature 60.0 - 150 °C
7980 - 15200 psi

@Temperature 140 - 302 °F
Average value: 59.8 MPa Grade Count:3
4.06 - 158.39 MPa

@Temperature -40.0 - 150 °C
589 - 22973 psi

@Temperature -40.0 - 302 °F
Average value: 59.8 MPa Grade Count:1
4.06 - 158.39 MPa

@Strain 0.100 - 5.00 %
589 - 22973 psi

@Strain 0.100 - 5.00 %
Average value: 59.8 MPa Grade Count:1
Elongation at Break 1.00 - 6.00 %
1.00 - 6.00 %
Average value: 2.28 % Grade Count:36
2.00 - 12.0 %

@Temperature 60.0 - 150 °C
2.00 - 12.0 %

@Temperature 140 - 302 °F
Average value: 5.48 % Grade Count:3
Elongation at Yield 3.50 - 10.0 %

@Temperature 120 - 150 °C
3.50 - 10.0 %

@Temperature 248 - 302 °F
Average value: 6.75 % Grade Count:1
Modulus of Elasticity 4.14 - 15.4 GPa
600 - 2230 ksi
Average value: 7.89 GPa Grade Count:34
2.00 - 6.80 GPa

@Temperature 60.0 - 150 °C
290 - 986 ksi

@Temperature 140 - 302 °F
Average value: 4.78 GPa Grade Count:3
Flexural Yield Strength 110 - 226 MPa
16000 - 32800 psi
Average value: 173 MPa Grade Count:28
66.9 - 141 MPa

@Temperature 100 - 100 °C
9700 - 20500 psi

@Temperature 212 - 212 °F
Average value: 104 MPa Grade Count:2
Flexural Modulus 3.45 - 9.65 GPa
500 - 1400 ksi
Average value: 6.85 GPa Grade Count:31
2.34 - 4.96 GPa

@Temperature 100 - 100 °C
339 - 719 ksi

@Temperature 212 - 212 °F
Average value: 3.65 GPa Grade Count:2
Compressive Yield Strength 100 - 207 MPa
14500 - 30000 psi
Average value: 155 MPa Grade Count:4
Shear Strength 44.1 - 88.0 MPa
6400 - 12800 psi
Average value: 67.4 MPa Grade Count:6
Izod Impact, Notched 0.180 - 2.14 J/cm
0.337 - 4.00 ft-lb/in
Average value: 0.563 J/cm Grade Count:25
Izod Impact, Unnotched 2.67 - 9.60 J/cm
5.00 - 18.0 ft-lb/in
Average value: 4.99 J/cm Grade Count:18
Izod Impact, Notched (ISO) 2.50 - 12.0 kJ/m²
1.19 - 5.71 ft-lb/in²
Average value: 6.75 kJ/m² Grade Count:6
5.00 - 6.00 kJ/m²

@Temperature -40.0 - -30.0 °C
2.38 - 2.86 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.67 kJ/m² Grade Count:3
Charpy Impact Unnotched 2.00 - 8.60 J/cm²
9.52 - 40.9 ft-lb/in²
Average value: 4.54 J/cm² Grade Count:12
1.70 - 4.00 J/cm²

@Temperature -30.0 - -20.0 °C
8.09 - 19.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 2.78 J/cm² Grade Count:4
Charpy Impact, Notched 0.350 - 1.10 J/cm²
1.67 - 5.24 ft-lb/in²
Average value: 0.636 J/cm² Grade Count:12
0.400 - 0.600 J/cm²

@Temperature -40.0 - -20.0 °C
1.90 - 2.86 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.529 J/cm² Grade Count:6
Thermal Properties Metric English Comments
CTE, linear 22.0 - 500 µm/m-°C
12.2 - 278 µin/in-°F
Average value: 83.0 µm/m-°C Grade Count:13
11.0 - 500 µm/m-°C

@Temperature 55.0 - 250 °C
6.11 - 278 µin/in-°F

@Temperature 131 - 482 °F
Average value: 122 µm/m-°C Grade Count:8
CTE, linear, Transverse to Flow 30.0 - 96.0 µm/m-°C
16.7 - 53.3 µin/in-°F
Average value: 70.1 µm/m-°C Grade Count:11
77.0 - 160 µm/m-°C

@Temperature 55.0 - 250 °C
42.8 - 88.9 µin/in-°F

@Temperature 131 - 482 °F
Average value: 121 µm/m-°C Grade Count:8
Melting Point 300 - 324 °C
572 - 615 °F
Average value: 309 °C Grade Count:15
Deflection Temperature at 0.46 MPa (66 psi) 220 - 318 °C
428 - 604 °F
Average value: 284 °C Grade Count:15
Deflection Temperature at 1.8 MPa (264 psi) 188 - 277 °C
370 - 531 °F
Average value: 250 °C Grade Count:29
Vicat Softening Point 215 - 275 °C
419 - 527 °F
Average value: 246 °C Grade Count:5
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:23
Oxygen Index 23.0 - 35.0 %
23.0 - 35.0 %
Average value: 27.2 % Grade Count:5
Electrical Properties Metric English Comments
Electrical Resistivity 1000 - 1.00e+16 ohm-cm
1000 - 1.00e+16 ohm-cm
Average value: 1.81e+15 ohm-cm Grade Count:19
Surface Resistance 1000 - 1.00e+15 ohm
1000 - 1.00e+15 ohm
Average value: 4.02e+14 ohm Grade Count:5
Dielectric Constant 3.90 - 5.20
3.90 - 5.20
Average value: 4.37 Grade Count:5
Dielectric Strength 16.5 - 42.0 kV/mm
419 - 1070 kV/in
Average value: 22.9 kV/mm Grade Count:6
Dissipation Factor 0.00600 - 0.0230
0.00600 - 0.0230
Average value: 0.0154 Grade Count:5
Comparative Tracking Index 550 - 600 V
550 - 600 V
Average value: 575 V Grade Count:8
Processing Properties Metric English Comments
Processing Temperature 296 - 340 °C
565 - 644 °F
Average value: 319 °C Grade Count:6
Melt Temperature 240 - 343 °C
464 - 650 °F
Average value: 323 °C Grade Count:30
Mold Temperature 65.0 - 180 °C
149 - 356 °F
Average value: 127 °C Grade Count:34
Drying Temperature 90.0 - 130 °C
194 - 266 °F
Average value: 108 °C Grade Count:27
Moisture Content 0.0300 - 0.200 %
0.0300 - 0.200 %
Average value: 0.0767 % Grade Count:23
Dew Point -31.7 - -28.9 °C
-25.0 - -20.0 °F
Average value: -30.4 °C Grade Count:9
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Average value: 92.1 MPa Grade Count:14
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved