Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.69 - 1.88 g/cc
0.0611 - 0.0679 lb/in³
Average value: 1.78 g/cc Grade Count:105
Water Absorption 0.000 - 0.200 %
0.000 - 0.200 %
Average value: 0.0415 % Grade Count:85
Moisture Absorption at Equilibrium 0.000 - 0.0500 %
0.000 - 0.0500 %
Average value: 0.0233 % Grade Count:9
Water Absorption at Saturation 0.000 - 0.0500 %
0.000 - 0.0500 %
Average value: 0.0362 % Grade Count:8
Particle Size 5.00 µm
5.00 µm
Average value: 5.00 µm Grade Count:14
Viscosity 1200 - 2.00e+7 cP

@Temperature 232 - 260 °C
1200 - 2.00e+7 cP

@Temperature 450 - 500 °F
Average value: 2.16e+6 cP Grade Count:53
1200 - 2.00e+7 cP

@Shear Rate 50.0 - 100 1/s
1200 - 2.00e+7 cP

@Shear Rate 50.0 - 100 1/s
Average value: 2.16e+6 cP Grade Count:53
Viscosity Test 0.850 - 170 cm³/g

@Temperature 30.0 - 30.0 °C
0.850 - 170 cm³/g

@Temperature 86.0 - 86.0 °F
Average value: 46.5 cm³/g Grade Count:7
Linear Mold Shrinkage 0.0100 - 0.0350 cm/cm
0.0100 - 0.0350 in/in
Average value: 0.0255 cm/cm Grade Count:29
Linear Mold Shrinkage, Transverse 0.00800 - 0.0300 cm/cm
0.00800 - 0.0300 in/in
Average value: 0.0226 cm/cm Grade Count:6
Melt Flow 0.500 - 40.0 g/10 min
0.500 - 40.0 g/10 min
Average value: 8.85 g/10 min Grade Count:96
Ash 0.000 - 5.00 %
0.000 - 5.00 %
Average value: 2.50 % Grade Count:4
Mechanical Properties Metric English Comments
Hardness, Rockwell R 62.0 - 115
62.0 - 115
Average value: 92.3 Grade Count:3
Hardness, Shore D 47.0 - 82.0
47.0 - 82.0
Average value: 72.0 Grade Count:62
Ball Indentation Hardness 62.0 - 105 MPa
8990 - 15200 psi
Average value: 92.5 MPa Grade Count:4
Tensile Strength, Ultimate 12.0 - 714 MPa
1740 - 104000 psi
Average value: 124 MPa Grade Count:86
1.00 - 39.0 MPa

@Temperature 50.0 - 100 °C
145 - 5660 psi

@Temperature 122 - 212 °F
Average value: 14.6 MPa Grade Count:6
1.00 - 39.0 MPa

@Strain 20.0 - 20.0 %
145 - 5660 psi

@Strain 20.0 - 20.0 %
Average value: 14.6 MPa Grade Count:6
Tensile Strength, Yield 11.7 - 141 MPa
1700 - 20500 psi
Average value: 42.0 MPa Grade Count:90
Elongation at Break 4.50 - 800 %
4.50 - 800 %
Average value: 175 % Grade Count:108
Elongation at Yield 2.00 - 25.0 %
2.00 - 25.0 %
Average value: 10.5 % Grade Count:76
Creep Strength 3.70 - 3.70 MPa

@Temperature 60.0 - 90.0 °C
537 - 537 psi

@Temperature 140 - 194 °F
Average value: 3.70 MPa Grade Count:4
3.70 - 3.70 MPa

@Time 360000 - 3.60e+6 sec
537 - 537 psi

@Time 100 - 1000 hour
Average value: 3.70 MPa Grade Count:4
Modulus of Elasticity 0.100 - 7.00 GPa
14.5 - 1020 ksi
Average value: 1.54 GPa Grade Count:94
0.0500 - 1.40 GPa

@Temperature 50.0 - 100 °C
7.25 - 203 ksi

@Temperature 122 - 212 °F
Average value: 0.422 GPa Grade Count:5
Tenacity 0.371 - 0.416 N/tex
4.20 - 4.71 g/denier
Average value: 0.380 N/tex Grade Count:5
Flexural Yield Strength 10.0 - 207 MPa
1450 - 30000 psi
Average value: 52.0 MPa Grade Count:48
Flexural Modulus 0.192 - 8.55 GPa
27.8 - 1240 ksi
Average value: 1.63 GPa Grade Count:56
Compressive Yield Strength 3.00 - 172 MPa
435 - 24900 psi
Average value: 51.2 MPa Grade Count:33
Izod Impact, Notched 0.400 - 5340 J/cm
0.749 - 10000 ft-lb/in
Average value: 3.00 J/cm Grade Count:60
Izod Impact, Unnotched 2.67 J/cm - NB
5.00 ft-lb/in - NB
Average value: 19.0 J/cm Grade Count:34
Charpy Impact Unnotched 25.5 J/cm² - NB
121 ft-lb/in² - NB
Average value: 26.5 J/cm² Grade Count:8
21.0 - 26.0 J/cm²

@Temperature -30.0 - -30.0 °C
99.9 - 124 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 22.8 J/cm² Grade Count:4
Charpy Impact, Notched 0.600 - 1000 J/cm²
2.86 - 4760 ft-lb/in²
Average value: 2.75 J/cm² Grade Count:13
0.500 - 1.10 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 5.24 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.700 J/cm² Grade Count:6
Tensile Impact Strength 140 - 210 kJ/m²
66.6 - 99.9 ft-lb/in²
Average value: 170 kJ/m² Grade Count:3
Coefficient of Friction 0.100 - 0.540
0.100 - 0.540
Average value: 0.262 Grade Count:63
Coefficient of Friction, Static 0.0500 - 0.550
0.0500 - 0.550
Average value: 0.291 Grade Count:55
Taber Abrasion, mg/1000 Cycles 5.00 - 33.0
5.00 - 33.0
Average value: 11.0 Grade Count:54
Thermal Properties Metric English Comments
CTE, linear 36.0 - 216 µm/m-°C
20.0 - 120 µin/in-°F
Average value: 139 µm/m-°C Grade Count:76
86.0 - 370 µm/m-°C

@Temperature -40.0 - 85.0 °C
47.8 - 206 µin/in-°F

@Temperature -40.0 - 185 °F
Average value: 185 µm/m-°C Grade Count:5
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
Average value: 100 µm/m-°C Grade Count:3
Specific Heat Capacity 1.17 - 1.90 J/g-°C
0.280 - 0.454 BTU/lb-°F
Average value: 1.30 J/g-°C Grade Count:53
1.60 - 1.60 J/g-°C

@Temperature 100 - 100 °C
0.382 - 0.382 BTU/lb-°F

@Temperature 212 - 212 °F
Average value: 1.60 J/g-°C Grade Count:21
Thermal Conductivity 0.110 - 0.300 W/m-K
0.763 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.182 W/m-K Grade Count:62
0.190 - 0.190 W/m-K

@Temperature 40.0 - 40.0 °C
1.32 - 1.32 BTU-in/hr-ft²-°F

@Temperature 104 - 104 °F
Average value: 0.190 W/m-K Grade Count:1
Melting Point 116 - 180 °C
240 - 356 °F
Average value: 161 °C Grade Count:117
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 5.00e+16 ohm-cm
100 - 5.00e+16 ohm-cm
Average value: 1.25e+15 ohm-cm Grade Count:86
Surface Resistance 100 - 1.00e+16 ohm
100 - 1.00e+16 ohm
Average value: 3.89e+14 ohm Grade Count:42
Dielectric Constant 3.20 - 33.5
3.20 - 33.5
Average value: 7.93 Grade Count:67
Dielectric Strength 10.0 - 150 kV/mm
254 - 3810 kV/in
Average value: 42.4 kV/mm Grade Count:58
Dissipation Factor 0.00500 - 0.370
0.00500 - 0.370
Average value: 0.124 Grade Count:48
Dielectric Loss Index 0.0250 - 0.165
0.0250 - 0.165
Average value: 0.100 Grade Count:3
Arc Resistance 50.0 sec
50.0 sec
Average value: 50.0 sec Grade Count:3
Comparative Tracking Index 250 - 600 V
250 - 600 V
Average value: 344 V Grade Count:4