Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers 20GF 20% Glass Fiber Reinforced ABS, Flame Retardant

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Manufacturer Oxford Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers 20GF 20% Glass Fiber Reinforced ABS, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Filler Content 20 %
20 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Temperature 23.0 °C
1.60 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D648
Users viewing this material also viewed the following: