Oxford Polymers 40GF 40% Glass Fiber Reinforced Polyphenylene Sulfide

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer Oxford Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers 40GF 40% Glass Fiber Reinforced Polyphenylene Sulfide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Glass Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Filler Content 40 %
40 %
Water Absorption 0.020 %
0.020 %
ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 131 MPa
19000 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 11.4 GPa
1650 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Temperature 23.0 °C
1.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C
210 °F
ASTM D648