Oxford Polymers 604-I Polycarbonate/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Oxford Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers 604-I Polycarbonate/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate/ABS AlloyInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Elongation at Break 145 %
145 %
ASTM D638
Flexural Strength 70.3 MPa
10200 psi
ASTM D790
Flexural Modulus 1.90 GPa
275 ksi
ASTM D790
Izod Impact, Notched 4.54 J/cm

@Temperature -40.0 °C
8.50 ft-lb/in

@Temperature -40.0 °F
ASTM D256
5.87 J/cm

@Temperature 23.0 °C
11.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
224 °F
ASTM D648