Oxford Polymers Oxnilon 66-13GF 13% Glass Fiber Filled Nylon 66 for Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Oxford Polymers
Trade Name Oxnilon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers Oxnilon 66-13GF 13% Glass Fiber Filled Nylon 66 for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
13% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Filler Content 13 %
13 %
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ASTM D638
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Temperature 23.0 °C
0.900 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
Deflection Temperature at 1.8 MPa (264 psi) 242 °C
468 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 288 - 304 °C
550 - 580 °F