Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers Oxnilon 66-50GF 50% Glass Fiber Filled Nylon 66 for Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Oxford Polymers
Trade Name Oxnilon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers Oxnilon 66-50GF 50% Glass Fiber Filled Nylon 66 for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.61 g/cc
1.61 g/cc
ASTM D792
Filler Content 50 %
50 %
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
ASTM D638
Tensile Strength, Yield 200 MPa
29000 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Strength 290 MPa
42000 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 293 - 304 °C
560 - 580 °F
Copyright © lookpolymers.com All Rights Reserved