Material Notes:
P & P Technology material reference EC-Q(F) is a fluorosilicone elastomer with a Nickel/Graphite conductive filler. Per MIL-G-83528. It is dark green in color. The material is specially compounded to offer excellent physical and electrical properties over an effective temperature range of –55°C to +160°C. Fluorosilicone offers excellent performance over a wide temperature range with good resistance to chemicals and weathering. It also has good resistance to most mineral oils and greases.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 3.25 g/cc
3.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
ASTM D2240
Tensile Strength 0.750 MPa
109 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Compression Set <= 30 %

@Temperature 100 °C,
Time 259000 sec
<= 30 %

@Temperature 212 °F,
Time 72.0 hour
ASTM D395
Electrical Properties Metric English Comments
Volume Resistivity <= 0.050 ohm-cm
<= 0.050 ohm-cm
Mil-G-83528
Shielding Effectiveness 101.5 - 112.6 dB
101.5 - 112.6 dB
Transfer Impedance; SEA ARP 1105
70 dB

@Frequency 200000 Hz
70 dB

@Frequency 200000 Hz
Mil std 285 procedure; Mil-G-83528
100 dB

@Frequency 1.00e+8 Hz
100 dB

@Frequency 1.00e+8 Hz
Mil std 285 procedure; Mil-G-83528
100 dB

@Frequency 5.00e+8 Hz
100 dB

@Frequency 5.00e+8 Hz
Mil std 285 procedure; Mil-G-83528
100 dB

@Frequency 2.00e+9 Hz
100 dB

@Frequency 2.00e+9 Hz
Mil std 285 procedure; Mil-G-83528
100 dB

@Frequency 1.00e+10 Hz
100 dB

@Frequency 1.00e+10 Hz
Mil std 285 procedure; Mil-G-83528