Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

P & P Technology ECF-J Silver Aluminum Loaded Fluorosilicone

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer P & P Technology
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology ECF-J Silver Aluminum Loaded Fluorosilicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
P & P Technology material reference ECF-J is a fluorosilicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical properties over an effective temperature range of –55 to +160°C. Fluorosilicone offers excellent performance over a wide temperature range with good resistance to hydrocarbons, chemicals and weathering. Its resistance to mineral based fluids is limited, but it has good splash resistance to most mineral oils and greases.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 2.00 - 2.20 g/cc
2.00 - 2.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 65
55 - 65
ASTM D2240
Tensile Strength 1.60 MPa
232 psi
ASTM D412
Elongation at Break >= 110 %
>= 110 %
ASTM D412
Compression Set <= 30 %

@Temperature 100 °C,
Time 259000 sec
<= 30 %

@Temperature 212 °F,
Time 72.0 hour
ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.012 ohm-cm
<= 0.012 ohm-cm
Mil-G-83528
Shielding Effectiveness 79 dB

@Frequency 200000 Hz
79 dB

@Frequency 200000 Hz
Mil-G-83528/Mil std 285
102 dB

@Frequency 2.00e+9 Hz
102 dB

@Frequency 2.00e+9 Hz
Mil-G-83528/Mil std 285
105 dB

@Frequency 1.00e+8 Hz
105 dB

@Frequency 1.00e+8 Hz
Mil-G-83528/Mil std 285
108 dB

@Frequency 5.00e+8 Hz
108 dB

@Frequency 5.00e+8 Hz
Mil-G-83528/Mil std 285
110 dB

@Frequency 1.00e+10 Hz
110 dB

@Frequency 1.00e+10 Hz
Mil-G-83528/Mil std 285