Material Notes:
P & P Technology conductive silver/aluminum adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exposed to atmospheric moisture.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 1.86 g/cc
1.86 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
Tensile Strength 1.79 MPa
260 psi
Elongation at Break >= 155 %
>= 155 %
Shear Strength >= 1.21 MPa
>= 175 psi
Tear Strength >= 45.0 kN/m
>= 257 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 400 °C
752 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.010 ohm-cm
0.010 ohm-cm
Processing Properties Metric English Comments
Cure Time 15.0 min
0.250 hour
Skin over
90.0 min
1.50 hour
Tack free
720 - 1440 min
12.0 - 24.0 hour
Cure for Handling
4320 - 8640 min
72.0 - 144 hour
Full Cure
Descriptive Properties Value Comments
Color Blue
Users viewing this material also viewed the following: